Environmentally-friendly decoration stone production method
A production method and stone technology, applied in the direction of surface coating liquid device, coating, pretreatment surface, etc., can solve the problems such as the lack of improvement in the structural strength of the plate, waste of stone resources, and difficult construction, etc., to achieve The effect of novel and bright appearance, simple production process and low cost
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0021] A method for making an environmentally friendly decorative stone, mainly comprising the following steps:
[0022] Step 1: Cut the raw material into a plate shape, roughen the layer that needs to be sprayed with paint through an automatic sandblasting machine, scrub the surface with a degreaser, and dehumidify it in an 80-degree drying room for one hour to let all the moisture inside the stone volatilize to achieve the best paint finish. good adhesion;
[0023] Step 2: paint bottom layer process: use unsaturated polyester resin to add fumed silica with a weight ratio of 20%-30% to make it muddy, add a weight ratio of 5% curing agent, and use a scraper to scrape on the surface to be sprayed with paint. The thickness of the scraping is less than 1 mm. If there are air bubbles infiltrated during the scraping, it must be scraped thoroughly with a scraper to ensure good adhesion. After the putty is scraped for 2-3 hours, first polish the surface with 120#-180# sandpaper , Gr...
Embodiment 2
[0031] A method for making an environmentally friendly decorative stone, mainly comprising the following steps:
[0032] Step 1: Cut the raw material into a plate shape, roughen the layer that needs to be sprayed with paint through an automatic sandblasting machine, scrub the surface with a degreaser, and dehumidify it in an 80-degree drying room for one hour to let all the moisture inside the stone volatilize to achieve the best paint finish. good adhesion;
[0033] Step 2: paint bottom layer process: use unsaturated polyester resin to add fumed silica with a weight ratio of 20%-30% to make it muddy, add a weight ratio of 5% curing agent, and use a scraper to scrape on the surface to be sprayed with paint. The thickness of the scraping is less than 1 mm. If there are air bubbles infiltrated during the scraping, it must be scraped thoroughly with a scraper to ensure good adhesion. After the putty is scraped for 2-3 hours, first polish the surface with 120#-180# sandpaper , Gr...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com