Embodiment 1
[0019] Example 1: Metal flower drying curved surface draping
[0020] A method for covering a curved surface of a metal flower drying product, comprising the following steps:
[0021] Step 1. Surface pretreatment:
[0022] Carry out surface pretreatment on the metal flower to remove the dust, grease and surface oxide of the metal flower;
[0023] Step two, nano-plating:
[0024] Prepare a surfactant solution, and spray the surfactant solution onto the surface of the metal flower; the preparation method of the surfactant solution is, for every 5 kilograms of activation solution prepared, take 76 grams of stannous chloride and a volume fraction of 38%. 59 milliliters of hydrochloric acid, 4750 milliliters of distilled water, above-mentioned three are mixed evenly, make activation solution, let stand for 8 hours, stand-by;
[0025] Prepare a nano-plating solution that does not contain silver nitrate, use a spray gun to spray the nano-plating solution onto the surface of the me...
Embodiment 2
[0028] The curved surface coating of embodiment 2 ceramic cup
[0029] A method for coating a curved surface of a ceramic cup, comprising the following steps:
[0030] Step 1. Surface pretreatment:
[0031] Surface pretreatment of ceramic cups to remove static electricity, dust and grease on the surface of ceramic cups;
[0032] Step two, nano-plating:
[0033] Prepare surfactant solution, surfactant solution is sprayed onto workpiece surface; The preparation method of described surfactant solution is, every preparation 5 kilograms of activation solutions, get 80 grams of tin protochloride, volume fraction is 38% hydrochloric acid 62 milliliter, 5000 milliliters of distilled water, mix the above three evenly to prepare the activation solution, let it stand for 8 hours, and set it aside.
[0034] Prepare a nano-plating solution that does not contain silver nitrate, use a spray gun to spray the nano-plating solution onto the surface of a ceramic cup, and perform conventional ...
Embodiment 3
[0036] The curved surface of embodiment 3 plastic pots is draped
[0037] A method for covering a curved surface of a plastic basin, comprising the following steps:
[0038] Step 1. Surface pretreatment:
[0039] Surface pretreatment of plastic basins to remove static electricity, dust and grease on the surface of plastic basins;
[0040] Step two, nano-plating:
[0041] Prepare surfactant solution, before spraying nano-plating solution, surfactant solution is sprayed on the surface of plastic basin; The preparation method of described surfactant solution is, every preparation 5 kilograms of activation solution, get 84 grams of tin protochloride , volume fraction is 67 milliliters of hydrochloric acid of 38%, 5250 milliliters of distilled water, above-mentioned three are mixed homogeneously, make activation solution, leave standstill for 8 hours, stand-by;
[0042]Prepare a nano-plating solution that does not contain silver nitrate, use a spray gun to spray the nano-plating...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com