Novel wear-resistant plastic barbell
A plastic and barbell technology, applied in the field of fitness equipment, can solve the problems of increasing economic burden, insufficient wear resistance, increasing bone density, etc., and achieves the effects of good wear resistance, high yield and not easy to crack
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0010] The novel wear-resistant plastic barbell of the present invention is made of the following components according to the weight ratio:
[0011] Proportion by weight fraction is made from the following components:
[0012] 15 parts of polyvinyl chloride resin, 3 parts of zinc oxide, 7 parts of calcium carbonate powder, 4 parts of latex powder, 6 parts of quartz powder, 3 parts of lauryl alcohol, 3 parts of stabilizer, 12 parts of low-pressure polyethylene, 7 parts of POE , 10 parts of tetraerythritol ester, 4 parts of paraffin, 25 parts of filler, 2 parts of tribasic lead sulfate, 7 parts of calcium carbonate, 6 parts of epoxy butyl stearate, 1 part of calcium stearate, dibasic sulfuric acid 4 parts of lead, 4 parts of dioctyl phthalate, 6 parts of lead stearate, 20 parts of polyethylene resin, 5 parts of carbon black, 3 parts of paraffin, 5 parts of sodium antimonate, 8 parts of nano silicon dioxide, three 2.5 parts of basic lead sulfate, 3 parts of dimethyl siloxane, 30...
Embodiment 2
[0014] The novel wear-resistant plastic barbell of the present invention is made of the following components according to the weight ratio:
[0015] Proportion by weight fraction is made from the following components:
[0016] 18 parts of polyvinyl chloride resin, 7 parts of zinc oxide, 9 parts of calcium carbonate powder, 10 parts of latex powder, 12 parts of quartz powder, 7 parts of lauryl alcohol, 8 parts of stabilizer, 23 parts of low-pressure polyethylene, 12 parts of POE , 14 parts of tetraerythritol ester, 6 parts of paraffin, 35 parts of filler, 4 parts of tribasic lead sulfate, 8 parts of calcium carbonate, 9.4 parts of epoxy butyl stearate, 3 parts of calcium stearate, dibasic sulfuric acid 8 parts of lead, 6 parts of dioctyl phthalate, 13 parts of lead stearate, 45 parts of polyethylene resin, 8 parts of carbon black, 4 parts of paraffin, 9 parts of sodium antimonate, 11 parts of nano silicon dioxide, three 7 parts of basic lead sulfate, 6 parts of dimethyl siloxa...
Embodiment 3
[0018] The novel wear-resistant plastic barbell of the present invention is made of the following components according to the weight ratio:
[0019] Proportion by weight fraction is made from the following components:
[0020] 16 parts of polyvinyl chloride resin, 5 parts of zinc oxide, 8 parts of calcium carbonate powder, 7 parts of latex powder, 9 parts of quartz powder, 5 parts of lauryl alcohol, 5 parts of stabilizer, 18 parts of low-pressure polyethylene, 9 parts of POE , 12 parts of tetraerythritol ester, 5 parts of paraffin, 30 parts of filler, 3 parts of tribasic lead sulfate, 7 parts of calcium carbonate, 8 parts of epoxy butyl stearate, 2 parts of calcium stearate, dibasic sulfuric acid 6 parts of lead, 5 parts of dioctyl phthalate, 9 parts of lead stearate, 32 parts of polyethylene resin, 7 parts of carbon black, 3 parts of paraffin, 7 parts of sodium antimonate, 9 parts of nano silicon dioxide, three 5 parts of basic lead sulfate, 4 parts of dimethyl siloxane, 37 ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com