Antiaging rubber
An anti-aging and anti-aging agent technology, applied in the rubber field, can solve the problems of rubber cracking and mold growth, and achieve the effect of avoiding cracking, slowing down the aging speed, and improving anti-aging.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0029] An anti-aging rubber, prepared from the following components: natural rubber SVR3L 70g, butadiene rubber 9000 30g, zinc oxide 8g, stearic acid 1.5g, ordinary paraffin 5g, microcrystalline wax 5g, coumarone resin 3g, 2g of coupling agent, 2g of dispersing aid, 8g of softener, 5g of anti-aging agent mixture, 1.3g of accelerator mixture, 80g of carbon black mixture, 2.5g of sulfur, and 0.2g of anti-scorch agent. Preferably, the antiaging agent mixture is antiaging agent RD and antiaging agent 4010NA, wherein the weight ratio of the two is: antiaging agent RD:antiaging agent 4010NA=2:3. The accelerator mixture is preferably accelerator CZ, accelerator DM, and accelerator TMTD, wherein the weight ratio of the three is: accelerator CZ: accelerator DM: accelerator TMTD=0.8:0.5:0.2. The carbon black mixture is preferably carbon black 330 and carbon black 774, wherein the weight ratio of the two is carbon black 330:carbon black 774=45:35. The coupling agent is preferably a sila...
Embodiment 2
[0040] An anti-aging rubber, prepared from the following components: natural rubber SVR3L 80g, butadiene rubber 9000 20g, zinc oxide 6g, stearic acid 2g, ordinary paraffin 6g, microcrystalline wax 4g, coumarone resin 4g, even 2.2g of joint agent, 4g of dispersing aid, 5g of softener, 6g of anti-aging agent mixture, 1.45g of accelerator mixture, 85g of carbon black mixture, 2g of sulfur, and 0.3g of anti-scorch agent. Preferably, the antiaging agent mixture is antiaging agent RD and antiaging agent 4010NA, wherein the weight ratio of the two is: antiaging agent RD:antiaging agent 4010NA=2.5:3.5. Preferably, the accelerator mixture is accelerator CZ, accelerator DM, and accelerator TMTD, and the weight ratio of the three is: accelerator CZ: accelerator DM: accelerator TMTD=1:0.3:0.3. The preferred carbon black mixture is carbon black 330 and carbon black 774, wherein the weight ratio of the two is carbon black 330:carbon black 774=50:30. The coupling agent is preferably a silan...
Embodiment 3
[0051] An anti-aging rubber, prepared from the following components: natural rubber SVR3L 90g, butadiene rubber 9000 10g, zinc oxide 5g, stearic acid 1g, ordinary paraffin 8g, microcrystalline wax 3g, coumarone resin 5g, even 3g of joint agent, 5g of dispersing aid, 10g of softener, 7g of anti-aging agent mixture, 1.8g of accelerator mixture, 70g of carbon black mixture, 1.8g of sulfur, and 0.4g of anti-scorch agent. Preferably, the antiaging agent mixture is antiaging agent RD and antiaging agent 4010NA, wherein the weight ratio of the two is: antiaging agent RD:antiaging agent 4010NA=3:4. Preferably, the accelerator mixture is accelerator CZ, accelerator DM, and accelerator TMTD, and the weight ratio of the three is: accelerator CZ: accelerator DM: accelerator TMTD=1.5:0.2:0.1. The carbon black mixture is preferably carbon black 330 and carbon black 774, wherein the weight ratio of the two is carbon black 330:carbon black 774=55:20. The coupling agent is preferably a silane...
PUM
Property | Measurement | Unit |
---|---|---|
elongation at break | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com