Rust inhibitor for industrial machinery and preparation method thereof
A technology for industrial machinery and rust inhibitor, applied in anti-corrosion coatings, coatings, etc., can solve problems affecting the appearance of materials, economic losses, environmental and human health hazards, etc., to ensure smoothness and smoothness, uniform composition, excellent The effect of anti-rust properties
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0020] An antirust agent for industrial machinery is composed of the following parts by mass: 2.5 parts of triethanolamine oleate, 4 parts of inorganic additives, 2 parts of sodium tetraborate, 0.8 parts of water-based nano-bentonite, 1.5 parts of zinc epoxy acid, fatty alcohol polyoxygen 3.5 parts of vinyl ether, 4 parts of dienyl succinimide, 1.5 parts of sodium lauroyl sarcosinate, 8 parts of n-butanol, 70 parts of water.
[0021] The inorganic additives are sodium silicate and sodium tungstate with a mass ratio of 1:1.
[0022] The preparation method of rust inhibitor for industrial machinery, the steps are as follows:
[0023] 1) Weigh the raw materials in parts by weight, heat and stir triethanolamine oleate, fatty alcohol polyoxyethylene ether, and sodium lauroyl sarcosinate for 20 minutes to obtain a mixed solution 1, the specific heating temperature is 75°C, and the stirring speed is 65rpm;
[0024] 2) Blend the mixed solution 1 with water-based nano-bentonite, zinc ...
Embodiment 2
[0028] An antirust agent for industrial machinery is composed of the following parts by mass: 1 part of triethanolamine oleate, 3 parts of inorganic additives, 2.5 parts of sodium tetraborate, 1.5 parts of water-based nano-bentonite, 3 parts of zinc epoxy acid, fatty alcohol polyoxygen 4 parts of vinyl ether, 1 part of dienyl succinimide, 4 parts of sodium lauroyl sarcosinate, 7 parts of n-butanol, 75 parts of water.
[0029] The inorganic additives are sodium silicate and sodium tungstate with a mass ratio of 1.5:1.
[0030] The preparation method of rust inhibitor for industrial machinery, the steps are as follows:
[0031] 1) Weigh the raw materials in parts by weight, heat and stir triethanolamine oleate, fatty alcohol polyoxyethylene ether, and sodium lauroyl sarcosinate for 15 minutes to obtain a mixed solution 1, the specific heating temperature is 75°C, and the stirring speed is 70rpm;
[0032] 2) Blend the mixed solution 1 with water-based nano-bentonite, zinc epoxy ...
Embodiment 3
[0036] An antirust agent for industrial machinery is composed of the following parts by mass: 3 parts of triethanolamine oleate, 3.5 parts of inorganic additives, 2 parts of sodium tetraborate, 2 parts of water-based nano-bentonite, 2.5 parts of zinc epoxy acid, fatty alcohol polyoxygen 4 parts of vinyl ether, 2 parts of dienyl succinimide, 3.5 parts of sodium lauroyl sarcosinate, 7 parts of n-butanol, 80 parts of water.
[0037] The inorganic additives are sodium silicate and sodium tungstate with a mass ratio of 1:1.
[0038] The preparation method of rust inhibitor for industrial machinery, the steps are as follows:
[0039] 1) Weigh the raw materials in parts by weight, heat and stir triethanolamine oleate, fatty alcohol polyoxyethylene ether, and sodium lauroyl sarcosinate for 20 minutes to obtain a mixed solution 1, the specific heating temperature is 75°C, and the stirring speed is 65rpm;
[0040] 2) Blend the mixed solution 1 with water-based nano-bentonite, zinc epox...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology