Environment-friendly interior wall putty with indoor humidity adjustment function
A technology for indoor humidity and interior wall putty, applied in the direction of filling slurry, etc., can solve the problems of easy shrinkage and cracking of cement-based materials, insufficient strength and hardness, and poor stability, and achieve strong adhesion and fast drying speed. , strong bonding effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0018] (1) Add 10 parts of vegetable starch to 50 parts of water, heat to 70-80°C for 30 minutes under constant stirring, then add 2 parts of sodium hydroxide and stir to dissolve completely, then add 25 parts of acrylic acid, 0.3 parts of diethylene Triamine and 0.2 parts of potassium persulfate, the mixture was heated to reflux state and kept stirring for 1 hour, and after naturally cooling to room temperature, it was sent into a freeze dryer, and the obtained solid was pulverized into powder to obtain material I;
[0019] (2) Add 5 parts of microcrystalline wax and 2 parts of nano rubber powder to 8 parts of disproportionated rosin, first heat to 80-90 ° C and mix for 10 minutes, then add 6 parts of ceramic micropowder, 8 parts of dodecyl alcohol ester and 5 parts of Carboresin, continue to heat to 120-130 ° C and mix for 10 minutes, and then naturally cool to room temperature to obtain material II;
[0020] (3) Add 10 parts of volcanic ash, 6 parts of fumed silica and 3 pa...
Embodiment 2
[0022] (1) Add 15 parts of vegetable starch to 60 parts of water, heat to 70-80°C for 30 minutes under constant stirring, then add 3 parts of sodium hydroxide and stir to dissolve completely, then add 25 parts of acrylic acid, 0.3 parts of diethylene Triamine and 0.2 parts of potassium persulfate, the mixture was heated to reflux state and kept stirring for 1 hour, and after naturally cooling to room temperature, it was sent into a freeze dryer, and the obtained solid was pulverized into powder to obtain material I;
[0023] (2) Add 3 parts of microcrystalline wax and 3 parts of nano rubber powder to 10 parts of disproportionated rosin, first heat to 80-90 ° C and mix for 10 minutes, then add 8 parts of ceramic micropowder, 6 parts of dodecyl alcohol ester and 6 parts of Carboresin, continue to heat to 120-130 ° C and mix for 10 minutes, and then naturally cool to room temperature to obtain material II;
[0024] (3) Add 10 parts of volcanic ash, 4 parts of fumed silica and 4 p...
PUM

Abstract
Description
Claims
Application Information

- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com