Waterborne polyurethane polymer modified concrete for bridge deck slab and preparation method
A water-based polyurethane and polymer technology, which is applied in the field of building materials, can solve problems such as bridge deck corrosion and damage, and achieve the effects of reducing the structural weight, improving compression resistance, and increasing the structural span
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0022] Example 1: 52.5 ordinary Portland cement, coarse aggregate with a maximum particle size of no more than 20mm, medium sand, fly ash, silica fume, concrete superplasticizer with β-naphthalenesulfonic acid formaldehyde condensate as the main component , water-based polyurethane with a solid content of 35% and water, these raw materials are as follows according to weight ratio: 16.8%, 29.8%, 39.8%, 2.7%, 1.5%, 0.2%, 7.2%, 2%.
[0023] At room temperature, put the dry aggregate and filler into the forced mixer and stir for 2 minutes. Then add the aqueous polyurethane emulsion and stir for another 3 minutes. Then water was added and stirred for 2 min. Finally, add naphthalene-based high-efficiency water reducer. Finally, add naphthalene-based high-efficiency water reducer and stir for 2 minutes to make the mixture reach a uniform state, and then construction can be carried out.
Embodiment 2
[0024] Example 2: 52.5 ordinary Portland cement, coarse aggregate with a maximum particle size of no more than 20mm, medium sand, fly ash, silica fume, concrete superplasticizer with β-naphthalenesulfonic acid formaldehyde condensate as the main component , the water-based polyurethane with a solid content of 35% and the raw materials of water are as follows according to the weight ratio: 18.9%, 31%, 36%, 3%, 1.8%, 0.25%, 5.4%, 3.65%.
[0025] At room temperature, put the dry aggregate and filler into the forced mixer and stir for 2 minutes. Then add the aqueous polyurethane emulsion and stir for another 3 minutes. Then water was added and stirred for 2 min. Finally, add naphthalene-based high-efficiency water reducer. Finally, add naphthalene-based high-efficiency water reducer and stir for 2 minutes to make the mixture reach a uniform state, and then construction can be carried out.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com