Water-based paint
A water-based coating and deionized water technology, applied in polyester coatings, coatings, etc., can solve the problems of poor solubility of raw materials, uneven dispersion, poor anti-pollution ability of coatings, etc., and achieve good impact resistance and uniform dispersion. , The effect of weather resistance and energy consumption
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0012] A water-based paint, characterized in that: comprising the following components by weight, 20 parts of alkyd resin, 12 parts of hydroxypropyl bromide resin, 15 parts of hydroxyethyl acrylate, 15 parts of isooctyl acrylate, diethyl malonate 8 parts of ester, 6 parts of methyl methacrylate, 3 parts of acrylic acid, 6 parts of talcum powder, 4 parts of calcite, 5 parts of titanium dioxide, 3 parts of dibutyltin dilaurate, 2 parts of 10% silicone oil, 2 parts of magnesium stearate , 0.5 parts of N,N-dimethylethanolamine, 1.6 parts of organic bentonite, 0.2 parts of lecithin, 2 parts of diluent, 6 parts of additives, 0.5 parts of propylene glycol methyl ether, and 55 parts of deionized water.
[0013] Further, the diluent is a mixture of propylene glycol methyl ether and isopropanol, and its weight ratio is 3:2.
[0014] Further, the auxiliary agent is a mixture of antiseptic, leveling agent and defoamer.
Embodiment 2
[0016] A water-based paint, characterized in that: comprising the following components by weight, 10 parts of alkyd resin, 8 parts of hydroxypropyl bromide resin, 15 parts of hydroxyethyl acrylate, 10 parts of isooctyl acrylate, diethyl malonate 3 parts of ester, 2 parts of methyl methacrylate, 3 parts of acrylic acid, 6 parts of talc, 4 parts of calcite, 10 parts of titanium dioxide, 2 parts of dibutyltin dilaurate, 0.1 part of 10% silicone oil, 2 parts of magnesium stearate , 0.5 parts of N,N-dimethylethanolamine, 1.6 parts of organic bentonite, 1.1 parts of lecithin, 8 parts of diluent, 2 parts of additives, 4 parts of propylene glycol methyl ether, and 35 parts of deionized water.
[0017] Further, the diluent is a mixture of propylene glycol methyl ether and isopropanol, and its weight ratio is 3:2.
[0018] Further, the auxiliary agent is a mixture of antiseptic, leveling agent and defoamer.
Embodiment 3
[0020] A water-based paint, comprising the following components by weight, 15 parts of alkyd resin, 10 parts of hydroxypropyl bromide resin, 12 parts of hydroxyethyl acrylate, 11 parts of isooctyl acrylate, 5 parts of diethyl malonate, 4 parts of methyl methacrylate, 3 parts of acrylic acid, 12 parts of talc, 10 parts of calcite, 6 parts of titanium dioxide, 2 parts of dibutyltin dilaurate, 1.6 parts of 10% silicone oil, 2.5 parts of magnesium stearate, N,N - 1.2 parts of dimethylethanolamine, 1.1 parts of organic bentonite, 0.8 parts of lecithin, 5 parts of diluent, 4 parts of additives, 2 parts of propylene glycol methyl ether, and 40 parts of deionized water.
[0021] Further, the diluent is a mixture of propylene glycol methyl ether and isopropanol, and its weight ratio is 3:2.
[0022] Further, the auxiliary agent is a mixture of antiseptic, leveling agent and defoamer.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com