Ultraviolet photocuring alkene unsaturated polyester coating for ceramic
A technology of polyester coatings and ultraviolet rays, which is applied in the field of coatings and can solve problems such as wear resistance, poor heat resistance, and intolerance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0015] An ultraviolet photocurable ethylenically unsaturated polyester coating for ceramics, its raw materials are proportioned as follows in parts by weight: 100 parts of bisphenol A butyl acetate glyceryl ether; 10 parts of carboxymethyl cellulose; 20 parts of acid; 5 parts of lithopone; 40 parts of butyl acetate; 10 parts of sanfei powder; 5 parts of benzophenone; 15 parts of talcum powder; 20 parts of acrylic acid; 1 part of ultramarine; 15 parts of sodium silicate; 25 parts of ethyl isocyanatomethacrylate; 20 parts of zinc oxide; 30 parts of dibutyltin dilaurate.
[0016] Heat the above raw materials in a reaction kettle to 70°C and stir for 12 hours. After mixing evenly, cool to room temperature and put them into a grinder to grind for 1 hour.
[0017] The gloss of the product is 110%, and there is no foaming or shedding after soaking in amyl acetate for 1 day; there is no abnormality in the friction of acetone and 5% ammonia soaked cotton balls for 24 hours; there is no...
Embodiment 2
[0019] An ultraviolet photocurable ethylenically unsaturated polyester coating for ceramics, its raw materials are proportioned as follows in parts by weight: 100 parts of bisphenol A butyl acetate glyceryl ether; 30 parts of carboxymethyl cellulose; 30 parts of acid; 25 parts of lithopone; 50 parts of butyl acetate; 20 parts of sanfei powder; 15 parts of benzoin ether; 25 parts of talcum powder; 35 parts of sodium; 35 parts of isocyanatoethyl methacrylate; 30 parts of zinc oxide; 40 parts of dibutyltin dilaurate.
[0020] Heat the above raw materials in a reaction kettle to 80°C and stir for 16 hours. After mixing evenly, cool to room temperature and put them into a grinder to grind for 2 hours.
[0021] The gloss of the product is 120%, and there is no foaming or shedding after soaking in amyl acetate for 2 days; it is resistant to acetone and 5% ammonia water and soaked in cotton balls for 36 hours, and there is no abnormality; Scrubbing 700 times.
Embodiment 3
[0023] An ultraviolet photocurable ethylenically unsaturated polyester coating for ceramics, its raw materials are proportioned as follows in parts by weight: 100 parts of bisphenol A butyl acetate glyceryl ether; 20 parts of carboxymethyl cellulose; 25 parts of acid; 15 parts of lithopone; 45 parts of butyl acetate; 15 parts of sanfei powder; 10 parts of benzoin ether; 20 parts of talcum powder; ; 30 parts of isocyanatoethyl methacrylate; 25 parts of zinc oxide; 35 parts of dibutyltin dilaurate.
[0024] Heat the above raw materials in a reaction kettle to 75°C and stir for 14 hours. After mixing evenly, cool to room temperature and put them into a grinder to grind for 1 hour.
[0025] The gloss of the product is 130%, and there is no foaming or shedding after soaking in amyl acetate for 3 days; there is no abnormality in the friction of acetone and 5% ammonia soaked cotton balls for 48 hours; there is no foaming, wrinkling and skin resistance in 95% ethanol solution for 36 h...
PUM
Property | Measurement | Unit |
---|---|---|
hardness | aaaaa | aaaaa |
gloss | aaaaa | aaaaa |
gloss | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com