Looking for breakthrough ideas for innovation challenges? Try Patsnap Eureka!

Large-membrane thickness PE electrostatic-sprayed paint

A technology of electrostatic spraying and film thickness, which is applied in the direction of polyester coatings and coatings, can solve the problems of high labor intensity, low efficiency, and poor conductivity of operators, and achieve the goals of reduced labor intensity, high efficiency, and lower resistivity. Effect

Inactive Publication Date: 2014-12-03
展辰新材料集团股份有限公司 +4
View PDF4 Cites 5 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0003] At present, the PE coatings on the market are high-resistivity polymers, and most of the development direction is to improve the high-temperature resistance. However, PE resin is a non-polar polymer compound with poor conductivity. The PE coating cannot be adsorbed on the furniture surface, and the edge of the back part of the furniture cannot absorb PE coating
Most of them are sprayed by compressed air method. In order to reduce the cost, a large amount of inactive thinner is generally added to the thinner to achieve the effect of thin film. When sprayed by air spray method, it is easy to cause paint mist to splash and serious waste of paint, resulting in damage to the Environmental pollution; at the same time, the labor intensity of the operators is high, the efficiency is low, and the labor protection of the operators is not in place, which affects their health. However, the existing PE coating electrostatic spraying construction cannot adsorb the PE coating on the furniture surface, and the edge of the back of the furniture cannot Absorption of PE coatings can not achieve satisfactory use effect

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0038] Formula: 80 parts of unsaturated polyester resin, 0.02 parts of polymerization inhibitor, 2 parts of talcum powder, 8 parts of transparent powder, 3 parts of zinc stearate, 2 parts of diacetone alcohol, 3 parts of styrene; anti-settling agent: A200 gas phase 0.3 parts of silicon dioxide, defoaming agent: 0.3 parts of EFKA2720 non-organic silicon defoaming agent, leveling agent: 0.3 parts of EFKA3777 fluorine-modified acrylate leveling agent, conductive agent: 0.3 parts of BYK ES80 conductive agent.

[0039] Production method: put in unsaturated polyester resin → add diacetone alcohol → add polymerization inhibitor → disperse uniformly at medium speed → add defoamer, leveling agent, conductive agent in turn → disperse at medium speed for 5 minutes → add talcum powder and transparent powder , Zinc stearate → disperse at medium speed for 30 minutes to fineness ≤ 55 microns → add styrene;

[0040] The appearance of the obtained high film thickness PE electrostatic spray coa...

Embodiment 2

[0042] Formula: 70 parts of unsaturated polyester resin, 0.02 parts of polymerization inhibitor, 5 parts of talcum powder, 15 parts of transparent powder, 3 parts of zinc stearate, 2 parts of diacetone alcohol, 3 parts of styrene; anti-settling agent: A200 gas phase 0.4 parts of silicon dioxide, defoaming agent: 0.3 parts of EFKA2720 non-organic silicon defoaming agent, leveling agent: 0.3 parts of EFKA3777 fluorine-modified acrylate leveling agent, conductive agent: 0.3 parts of BYK ES80 conductive agent;

[0043] Production method: with embodiment 1;

[0044] The appearance of the obtained high film thickness PE electrostatic spray coating is: translucent, yellowish viscous liquid.

Embodiment 3

[0046] Formula: 60 parts of unsaturated polyester resin, 0.02 parts of polymerization inhibitor, 5 parts of talcum powder, 20 parts of transparent powder, 3 parts of zinc stearate, 2 parts of diacetone alcohol, 3 parts of styrene; anti-settling agent: A200 gas phase 0.5 parts of silicon dioxide, defoaming agent: 0.3 parts of EFKA2720 non-organic silicon defoaming agent, leveling agent: 0.2 parts of EFKA3777 fluorine-modified acrylate leveling agent, conductive agent: 0.2 parts of BYK ES80 conductive agent;

[0047] Production method: with embodiment 1;

[0048] The appearance of the obtained high film thickness PE electrostatic spray coating is: translucent, yellowish viscous liquid.

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

PropertyMeasurementUnit
tack-free timeaaaaaaaaaa
adhesivityaaaaaaaaaa
Login to View More

Abstract

The invention discloses large-membrane thickness PE electrostatic-sprayed paint. The large-membrane thickness PE electrostatic-sprayed paint comprises a main agent part A, a cobalt iso-octoate-containing part B and a methylethyl ketone peroxide-containing part C. The main agent part A comprises, by weight, 60-80 parts of unsaturated polyester resin, 0.01-0.03 parts of a polymerization inhibitor, 10-25 parts of an inorganic filling material, 3-5 parts of zinc stearate, 4-8 parts of a solvent, 0.3-0.5 parts of an anti-settling agent, 0.1-0.3 parts of an antifoaming agent, 0.2-0.5 parts of a leveling agent and 0.1-0.5 parts of a conductive agent which is an alkanolamide solution of nonsaturated acidic carboxylate. The alkanolamide solution of nonsaturated acidic carboxylate reduces paint resistance, improves paint conductivity and satisfies electrostatic-coating resistor requirements.

Description

technical field [0001] The invention relates to a PE paint, in particular to a PE electrostatic spray paint with high film thickness. Background technique [0002] Because of its solvent-free, high solid content, and good filling properties, PE coatings can be coated thickly at one time, with plump coating films, high hardness, excellent chemical resistance, low VOC emissions, and excellent filling properties in solid wood furniture and veneer furniture. The anti-slump performance is unmatched by PU primers. In recent years, it has developed very rapidly. The demand in the Chinese market has increased by 10% per year. It is gradually replacing PU primers and widely used in furniture coating. [0003] At present, the PE coatings on the market are high-resistivity polymers, and most of the development direction is to improve the high-temperature resistance. However, PE resin is a non-polar polymer compound with poor conductivity. The PE coating cannot be adsorbed on the surfa...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Applications(China)
IPC IPC(8): C09D167/06C09D7/12C09D5/46
Inventor 王琦陈寿生
Owner 展辰新材料集团股份有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Patsnap Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Patsnap Eureka Blog
Learn More
PatSnap group products