An enameled wire varnish and additive technology, applied in the field of enamelled wire varnish, can solve the problems of heat resistance lower than 120°C, difficult to meet different environments, poor wear resistance, etc., achieve good aging resistance, firm adhesion and not easy to peel off, paint membrane water resistance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment Construction
[0014] The wire enamelled varnish is made of the following raw materials in parts by weight (kg): 5 isocyanate, 7 ditetradecyl alcohol ester, 12 epoxy phenolic resin, 8 polyester acrylate, crosslinking agent TAC 2, tributyl Tin trichloride 2, nylon 12 14, 582-2 amino resin 6, dimethyl silicone oil 0.5, nano brick slag powder 3, potassium tetraborate 2, additive 7, m-p-cresol 120, xylene 100;
[0015] The auxiliary agent is made of the following raw materials in parts by weight (kg): 0.2 nanometer mica powder, 3 pentaerythritol, 4 glycerin, 2 isopropyl dioleate (dioctyl phosphate acyloxy) titanate, Crosslinking agent TAC2, dipentaerythritol hexaacrylate 7, triethyl citrate 7, propyl gallate 2, coix seed oil 3; the preparation method is to mix the materials, heat to 60-70°C, and stir for 30-40 Minutes and it's ready.
[0016] The preparation method comprises the following steps:
[0017] (1) Weigh xylene and m-p-cresol into a reaction kettle with a stirrer, stir and mix evenly...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com