A technology for sealing materials and building components, applied in the field of building materials and building construction, can solve the problems of high labor intensity, inability to withstand heat for a long time, poor adhesion, etc., and achieve the effects of good construction performance, long operation time and increased strength
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0056]
[0057] Preparation method: Weigh various raw materials according to the formula, and add quartz sand, cement (P.O42.5 ordinary Portland cement), active admixture (slag micropowder, silica fume), water reducer (poly Carboxylic acid superplasticizer), coagulant (sodium aluminate), expansion agent (ZY expansion agent), binder (vinyl acetate / ethylene copolymer powder binary copolymer powder), plastic retainer (lignocellulose , bentonite), starch ether and thixotropic lubricant, fully stirred evenly, and packaged to form a product.
[0058] The construction method is the same as before, wherein the amount of water added is 13% of the weight of the sealing material.
[0059] The sealing material prepared from the above-mentioned components according to the aforementioned process has the characteristics of moderate setting time, high strength, good plasticity and good anti-falling and sliding properties, and is suitable for the construction of splicing joints of general c...
Embodiment 2
[0061]
[0062] Preparation method: Weigh various raw materials according to the formula, and add quartz sand, cement (P.II52.5 Portland cement, aluminate cement CA-50), active admixture (slag powder), Water reducing agent (naphthalene-based high-efficiency water reducing agent), early strength agent (calcium formate), coagulation regulator (sodium carbonate), expansion agent (UEA expansion agent), binder (vinyl acetate / ethylene copolymer powder binary Copolymerized rubber powder, ethylene / vinyl laurate / vinyl chloride ternary copolymerized rubber powder), plastic retainer (methyl cellulose, diatomaceous earth), thixotropic lubricant, modified starch ether, fully stirred evenly, and packaged product.
[0063] The construction method is the same as before, wherein the amount of water added is 11% of the weight of the sealing material.
[0064] The sealing material prepared by the above components according to the aforementioned process has the characteristics of short settin...
Embodiment 3
[0066]
[0067] Preparation method: Weigh various raw materials according to the formula, and add quartz sand, cement (sulfoaluminate rapid hardening cement), active admixture (silica fume), and water reducer (melamine water reducer) to the stirring machine in sequence , early strength agent (sodium silicate, coagulation agent (sodium tetraborate), expansion agent (calcium oxide), binder (polyvinyl alcohol), plastic retainer (hydroxyethyl cellulose ether), thixotropic lubricant , fully stirred evenly, and packaged to form a product.
[0068] The construction method is the same as before, wherein the amount of water added is 16% of the weight of the sealing material.
[0069] The sealing material prepared from the above components according to the aforementioned process has the characteristics of short setting time, high early strength, good plasticity, and good anti-falling and sliding properties, and is suitable for the construction of fast sealing treatment of splicing jo...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com