Compound nano-silver emulsifiable paste and preparation method thereof
A technology of nano silver and silver cream, which is applied in the field of medicine to restore the health of the wounded, promote wound healing, and reduce combat attrition.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0039] Components and content of compound nano silver cream: 59.1g stearic acid, 59.1g stearyl alcohol, 118.2g liquid paraffin, 0.5g ethylparaben, 4.6g triethanolamine, 10.1g laurocaprolactone, 2,6 - 0.5g of di-tert-butyl-p-cresol, 0.5g of disodium edetate, 228g of glycerin, 232.6mL of nano-silver solution, 40g of zinc oxide, and add water to 1000g.
[0040] Preparation:
[0041] (1) Preparation of water phase: Add zinc oxide, glycerin, disodium edetate and ethylparaben to an appropriate amount of nano-silver solution, heat to 80°C, stir well, and set aside.
[0042] (2) Oil phase preparation: Mix stearic acid, stearyl alcohol, 2,6-di-tert-butyl-p-cresol, laurocaprazine and liquid paraffin, heat to 75°C, and stir well.
[0043] (3) Immediately add the water phase to the oil phase, then add triethanolamine, stop heating, and immediately stir rapidly, when the temperature drops to 50°C, continue stirring until it coagulates, and the compound nano silver cream is obtained.
Embodiment 2
[0045] The composition and content of the compound nano silver cream: stearic acid 59.1g, stearyl alcohol 59.1g, liquid paraffin 118.2g, triethanolamine 4.6g, glycerin 228g, nano silver liquid 200mL, zinc oxide 50g, add water to 1000g.
[0046] Preparation:
[0047] (1) Preparation of water phase: Mix glycerin and nano-silver solution, heat to 80°C, stir well, and set aside.
[0048] (2) Preparation of oil phase: Mix stearic acid, stearyl alcohol and liquid paraffin, heat to 75°C, stir well, and set aside.
[0049] (3) Immediately add the water phase to the oil phase, then add triethanolamine, stir until the emulsification is complete, add zinc oxide fine powder in stages, stir evenly, let cool to room temperature, and obtain the compound nano silver cream.
Embodiment 3
[0051] Components and content of compound nano silver cream: 59.1g stearic acid, 59.1g stearyl alcohol, 118.2g liquid paraffin, 4.6g triethanolamine, 10.1g laurocaprazine, 2,6-di-tert-butyl p-methyl 0.5g of phenol, 0.5g of disodium edetate, 228g of glycerin, 300mL of nano-silver solution, 45g of zinc oxide, and add water to 1000g.
[0052] Preparation:
[0053] (1) Preparation of water phase: Mix glycerin, disodium ethylenediaminetetraacetic acid, and nano-silver solution, heat to 80°C, stir well, and set aside.
[0054] (2) Oil phase preparation: Mix stearic acid, stearyl alcohol, 2,6-di-tert-butyl-p-cresol, laurocaprazine and liquid paraffin, heat to 75°C, stir well, and set aside.
[0055] (3) Then slowly add the water phase to the oil phase, stir as you add, then add triethanolamine until the emulsification is complete, add zinc oxide fine powder in stages, stir evenly, and cool to room temperature to obtain the compound nano silver cream .
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com