Method for manufacturing outer bag paper of fruit raising bags by using adherography
A fruit growing bag and offset printing technology, applied in the field of papermaking, can solve the problems of slow speed, large pollution, and large amount of carbon black used, and achieve the effects of fast speed, good strength and softness, and enhanced resistance to liquid penetration.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0013] 1) Preparation of water-repellent paraffin wax emulsion: Add 80 parts of paraffin wax and 15 parts of stearic acid into the reactor in parts by mass and heat at 60°C, then add 8 parts of borax and 1 part of soda ash, stir well, add 1200 dilute with water, and stir at 50°C for 1 hour to obtain a water-repellent paraffin emulsion;
[0014] 2) Base paper making: 50% of waste newspaper pulp with a beating degree of 40 to 50°SR and 50% of natural softwood pulp with a beating degree of 28 to 40°SR are mixed to obtain a mixture by mass percentage, and the mixture is added to To the tune-up pool and add relative to the quality of fiber dry pulp: 10% china clay, 1% rosin glue, 8% water-repelling agent paraffin wax emulsion, 3% wet strength agent PAE and 3% aluminum sulfate; Partial forming, pressing and dehydration, and drying to obtain outer bag paper base paper, the basis weight is 45g / m 2 ;
[0015] 3) The deployment of black ink: take 10% carbon black by mass percentage an...
Embodiment 2
[0018] 1) Preparation of water-resistant paraffin wax emulsion: Add 120 parts of paraffin and 30 parts of stearic acid into the reactor by mass parts and heat at 70°C, then add 9 parts of borax and 1.5 parts of soda ash, stir well, add 1800 Dilute with water, stir at 70°C for 2 hours to obtain water-resistant paraffin wax emulsion;
[0019] 2) base paper making: 70% of waste newspaper pulp with a beating degree of 40 to 50°SR and 30% of natural softwood pulp with a beating degree of 28 to 40°SR are mixed to obtain a mixture by mass percentage, and the mixture is added to To the tune into the pool and add relative to the quality of fiber dry pulp: 10% china clay, 1.5% rosin glue, 8% water-resistant agent paraffin wax emulsion, 3% wet strength agent PAE and 5% aluminum sulfate; Partial forming, pressing and dehydration, and drying to obtain outer bag paper base paper, the basis weight is 45g / m 2 ;
[0020] 3) The deployment of black ink: get 12% carbon black by mass percentage...
Embodiment 3
[0023] 1) Preparation of water-resistant paraffin wax emulsion: add 160 parts of paraffin and 40 parts of stearic acid into the reactor by mass parts and heat at 80°C, then add 10 parts of borax and 2 parts of soda ash, stir well, add 2300 dilute with water, and stir at 60°C for 1 hour to obtain a water-repellent paraffin emulsion;
[0024] 2) Base papermaking: 80% of waste newspaper pulp with a beating degree of 40 to 50°SR and 20% of natural softwood pulp with a beating degree of 28 to 40°SR are mixed to obtain a mixture by mass percentage, and the mixture is added to To the tune into the pool and add relative to the quality of fiber dry pulp: 10% of china clay, 2% of rosin glue, 8% of water-repelling agent paraffin wax emulsion, 3% of wet strength agent PAE and 4% of aluminum sulfate; Partial forming, pressing and dehydration, and drying to obtain outer bag paper base paper, the basis weight is 45g / m 2 ;
[0025] 3) The deployment of black ink: get 14% carbon black by mas...
PUM
Property | Measurement | Unit |
---|---|---|
opacity | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com