A self-replenishing and tire technology, applied in other chemical processes, chemical instruments and methods, etc., can solve problems such as tire blowout, valve blockage, economic loss, etc., and achieve the effect of preventing tire blowout, preventing air pressure drop, and improving economic benefits
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0018] A tire self-healing agent is composed of the following raw materials in parts by weight:
[0019] 3 parts of polyvinyl alcohol, 4 parts of copper sulfate, 5 parts of sodium nitrite, 2 parts of cellulose, 4 parts of gypsum powder, 2 parts of refined wood powder, 1 part of organic bentonite, 1.5 parts of water;
[0020] The preparation process of the tire self-healing agent is carried out according to the following steps:
[0021] A. After heating water and polyvinyl alcohol to 80°C, stop heating, stir it for 3 hours, then filter, then add cellulose, fine wood powder, organic bentonite and stir for 5 minutes;
[0022] B. Add gypsum powder, copper sulfate and sodium nitrite in step A, continue to stir for 0.5 hour, and pack it in a plastic container to obtain the finished product.
Embodiment 2
[0024] A tire self-healing agent is composed of the following raw materials in parts by weight:
[0025] 6 parts of polyvinyl alcohol, 5 parts of copper sulfate, 8 parts of sodium nitrite, 4 parts of cellulose, 5 parts of gypsum powder, 2 parts of refined wood powder, 2 parts of organic bentonite, 2 parts of water;
[0026] The preparation process of the tire self-healing agent is carried out according to the following steps:
[0027] A. After heating water and polyvinyl alcohol to 85°C, stop heating, stir it for 3 hours, then filter, then add cellulose, fine wood powder, organic bentonite and stir for 6 minutes;
[0028] B. Add gypsum powder, copper sulfate and sodium nitrite in step A, continue to stir for 0.5 hour, and pack it in a plastic container to obtain the finished product.
Embodiment 3
[0030] A tire self-healing agent is composed of the following raw materials in parts by weight:
[0031] 5 parts of polyvinyl alcohol, 6 parts of copper sulfate, 8 parts of sodium nitrite, 3 parts of cellulose, 5 parts of gypsum powder, 3 parts of refined wood powder, 2 parts of organic bentonite, 2 parts of water;
[0032] The preparation process of the tire self-healing agent is carried out according to the following steps:
[0033] A. After heating water and polyvinyl alcohol to 85°C, stop heating, stir it for 4 hours, then filter, then add cellulose, fine wood powder, organic bentonite and stir for 8 minutes;
[0034] B. Add gypsum powder, copper sulfate and sodium nitrite in step A, continue to stir for 1 hour, and pack it in a plastic container to obtain the finished product.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com