Water soluble alkyd resin-wax composite coating release-controlling fertiliser and method for preparing same
A technology of alkyd resin and controlled-release fertilizer, which is applied in the field of materials and fertilizers, can solve the problem that the dissolved polymer film is not easy to degrade, and achieve the effect of excellent controlled-release performance, good controlled-release performance, and low dependence
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0026] In a further preferred preparation method, firstly, fatty acids, polyols and dibasic acids (and / or their anhydrides) derived from plants are added to a reactor equipped with a stirrer, a reflux condenser, a thermometer and a nitrogen protection, and the temperature is 160~260 ℃ of reaction 0.5~6 hour, preferably 200~240 ℃ of reaction 2~4 hours, and remove the water that generates in the reaction with the water eliminator in time, then cool down to 120~200 ℃, add other polybasic acid (and / or its acid anhydride), the reaction is kept for at least 0.5 hours, and the water generated in the reaction is removed in time with a water eliminator. Optionally, add 2-20% by weight of rosin based on the total weight of the resin, preferably 3-10% by weight when the temperature is lowered to 130-160°C, and react at this temperature for 5 minutes to 2 hours, preferably 10 minutes to 0.5 hours . After cooling down, an alkyd resin prepolymer with a certain acid value is obtained. (2) ...
Embodiment 1
[0050] (1) Preparation of water-soluble alkyd resin coating agent
[0051] 480 grams of linseed oil, 236 grams of trimethylolpropane and 166 grams of isophthalic acid were added to the reactor equipped with a stirrer, reflux condenser, thermometer and nitrogen protection, and the temperature was raised to 235 ° C for 3.5 hours, and then the temperature was lowered. To 175 ° C, add 73 grams of trimellitic anhydride, react at this temperature for about 3 hours, and use a water eliminator to remove the water generated in the reaction in time, when the acid value of the system reaches 62 mgKOH / g resin, reduce the system temperature to 150 ° C, add 49 grams of rosin was reacted for 20 minutes.
[0052] Above-mentioned reaction system is cooled, when temperature is reduced to 70 ℃, add 70 grams of mixed solutions formed by ethylene glycol monobutyl ether and isopropanol (the weight ratio of the two is 1: 1.5) and mix well, drop to 50 ℃ In the following, the pH of the system was adj...
Embodiment 2
[0057] Same as Example 1, the difference is that diatomaceous earth is not used.
[0058] Calculated by dry matter weight, the obtained water-soluble alkyd resin-wax composite coated controlled-release fertilizer is composed of 89.6% of urea, 9% of polymer and 1.4% of paraffin. The nutrient release period of this controlled release fertilizer is 52 days.
PUM
Property | Measurement | Unit |
---|---|---|
acid value | aaaaa | aaaaa |
acid value | aaaaa | aaaaa |
acid value | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com