Composition formed from chitosan and its derivatives and low-molecular heparin and pneparation and preparing method
A technology of low-molecular-weight heparin and chitosan, which is applied in the direction of medical preparations, drug combinations, and pharmaceutical formulations of non-active ingredients, can solve problems such as difficult gastrointestinal mucosal absorption, poor patient compliance, and large molecular weight, and achieve reduction Effects of side effects, improvement of curative effect, and stability improvement
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0016] Example 1: Preparation of low-molecular-weight heparin and chitosan nano / micro-composites with different molecular weights: weigh chitosan with different molecular weights according to the above ratio to make a solution of appropriate concentration, and weigh low-molecular heparin according to the above ratio to make a suitable solution. The solution of the above concentration is added into the above-mentioned chitosan solution under the condition of stirring, the stirring is continued for 10 minutes, the stirring is stopped, and the solution is incubated at room temperature for 30 minutes to obtain the final product.
Embodiment 2
[0017] Example 2: Preparation of low-molecular-weight heparin and trimethyl chitosan nano / micro composites of different molecular weights: take trimethyl chitosan with different molecular weights according to the above ratio to make a solution of appropriate concentration, and weigh according to the above ratio Low-molecular-weight heparin is prepared into a solution with an appropriate concentration, added into the above-mentioned trimethyl chitosan solution under agitation, continued to agitate for 10 minutes, stopped agitation, and incubated at room temperature for 30 minutes to obtain the product.
Embodiment 3
[0018] Embodiment 3: Preparation of low molecular weight heparin and chitosan nano / micro composites of different molecular weight pegylated chitosan: take the chitosan of different molecular weight pegylated according to the above ratio to make a solution of appropriate concentration, press The above ratio is weighed with low molecular weight heparin to prepare a solution of appropriate concentration, added to the above-mentioned PEGylated chitosan solution under stirring conditions, continued to stir for 10 minutes, stopped stirring, and incubated at room temperature for 30 minutes to obtain.
PUM
Property | Measurement | Unit |
---|---|---|
Average molecular weight | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com