A drug coating and drug technology, which can be used in drug combinations, pharmaceutical formulations, medical preparations with inactive ingredients, etc., can solve problems such as stents affecting the efficacy of PTA, avoid the risk of delayed thrombosis, prevent restenosis, Reduces the effect of neointima formation
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0021] Add 0.20g of polybutylmethacrylate and 0.20g of ethylene-vinyl acetate copolymer into 10ml of trichloroethane, mix and disperse evenly, then add 0.10g of paclitaxel, disperse evenly at room temperature, and then spray on the surface of the stent. Cured in air for 60min. Repeat the above operation until the drug loading reaches 50 μg / cm 2 . The scaffolds were then dried in a vacuum oven. The mixture of parylene and cilostazol was coated on the outside of the drug-loaded layer by vapor deposition with a thickness of 1 μm.
Embodiment 2
[0023] Add an appropriate amount (eg 0.10g) of polylactic acid (PLA) and 0.10g of polycaprolactone (PCL) into 10ml of trichloroethane, mix and disperse evenly, then add 0.10g of paclitaxel, disperse evenly at room temperature, and then spray on bracket surface. Cured in air for 60min. Repeat the above operations until the drug loading reaches 400 μg / cm 2 . The scaffolds were then dried in a vacuum oven. The mixture of parylene and ticlopidine was coated on the outside of the drug-loaded layer by vapor deposition, and the thickness was controlled at 0.01 μm.
Embodiment 3
[0025] Add appropriate amount such as 0.20g polybutylmethacrylate and 0.20g ethylene-vinyl acetate copolymer to 10ml trichloroethane, mix and disperse evenly, then add 0.075g Cilostazol and 0.10g paclitaxel, disperse evenly under room temperature, then Spray on the surface of the bracket. Cured in air for 30min. Repeat the above operations until the weight of the drug-loaded layer reaches 200 μg / cm 2 . Then the stent was placed in a vacuum oven at 30° C. and vacuumed for 24 hours. In order to prevent the adhesion between the drug coating and the balloon, a layer of Parylene or its derivatives can be coated on the surface of the stent by vapor deposition, with a thickness of 10 microns.
PUM
Property | Measurement | Unit |
---|---|---|
thickness | aaaaa | aaaaa |
thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com