A technology of molten salt electrolysis and beryllium oxide, which is applied in the field of beryllium metallurgy, can solve problems such as difficult oxygen diffusion, oxygen generation, and serious equipment corrosion, and achieve the effects of shortening the process flow, mature and stable process, and improving direct yield
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0037] A method for preparing metal beryllium by electrolysis of beryllium oxide in molten fluoride salts, comprising the following steps:
[0038] Construct BeF with 25 at.% beryllium fluoride and 70.5 at.% lithium fluoride 2 -LiF molten salt system, mix well and put it into a nickel crucible, heat it to 880°C, then add 4.5 at.% granular beryllium oxide with a purity of 95%, use the nickel crucible as the cathode, graphite as the anode, and the pole distance is 3.0 cm, under a helium atmosphere, control the cathode voltage at -1.90V (vs NHE) for pre-electrolysis, make the content of impurity elements Fe, Al, and Si 2 , cathode current density 0.125A / cm 2 , Electrolyzed for 12 hours, metal beryllium particles with a purity of 99.3% were deposited on the cathode (most of the particles were less than 1mm, and the maximum was 3mm).
Embodiment 2
[0040] A method for preparing metal beryllium by electrolysis of beryllium oxide in molten fluoride salts, comprising the following steps:
[0041] Construct BeF with 45.35 at.% beryllium fluoride and 54.60 at.% lithium fluoride 2-LiF molten salt system, mix well and put it into a nickel crucible, heat it to 700°C, then add 0.05at.% granular beryllium oxide with a purity of 98.5%, use nickel mesh as the cathode, graphite as the anode, the cathode is on the bottom, and the anode On the top, the pole distance is 10.0cm, the cathode voltage is controlled at -1.88V (vs NHE) for pre-electrolysis, so that the content of impurity elements Fe, Al, and Si is 2 , cathode current density 0.18A / cm 2 , Electrolyzed for 12 hours, dendritic metal beryllium particles with a purity of 99.5% were precipitated on the cathode.
Embodiment 3
[0043] A method for preparing metal beryllium by electrolysis of beryllium oxide in molten fluoride salts, comprising the following steps:
[0044] Construct BeF with 40.2 at.% beryllium fluoride and 56.8 at.% potassium fluoride 2 -KF molten salt system, mix well and put it into an iron crucible, heat it to 740°C, then add 3.0 at.% granular beryllium oxide with a purity of 95%, use the iron crucible as the cathode, graphite as the anode, and the pole distance is 45.0 cm, under a helium atmosphere, control the cathode voltage at -1.8V (vs NHE) for pre-electrolysis, make the content of impurity elements Fe, Al, and Si 2 , cathode current density 0.85A / cm 2 , Electrolyzed for 5h, the rod-shaped metal beryllium with a purity of 99.2% was precipitated on the cathode.
PUM
Property | Measurement | Unit |
---|---|---|
purity | aaaaa | aaaaa |
purity | aaaaa | aaaaa |
purity | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com