preparation example Construction
[0073] Further, such as figure 2 As shown, the embodiment of the present invention also provides a preparation method of a drug balloon, comprising the following steps:
[0074] Step S11: providing a balloon body 1; the present invention does not limit the structure of the balloon body 1;
[0075] Step S12: setting the bottom layer 2 on the outer surface of the balloon body;
[0076] Step S13: setting the drug-loaded layer 3 on the surface of the bottom layer 2;
[0077] Step S14: setting the functional layer 4 on the surface of the drug-loaded layer 3 .
Embodiment 1
[0080]First, take 5 balloon catheters of 3.0mm*20mm (diameter*length), the material of each balloon catheter is Pebax (block polyether amide), and do the following for each balloon catheter:
[0081] Step 1: Wipe the surface of the balloon with 75% ethanol and set aside.
[0082] Step 2: Use plasma cleaning technology to clean the debris on the surface of the balloon. The plasma cleaning time is 15 minutes; the plasma cleaning technology uses argon as an inert gas, the power is 100KHz, and the pressure in the working chamber is 0.3atm during cleaning.
[0083] Step 3: Using dextran as the bottom layer material, spray a layer of dextran bottom layer with a molecular weight of 150K on the surface of the balloon, and the thickness of the bottom layer is 0.1 μm.
[0084] Step 4: Dissolve 500 mg of rapamycin and 5 g of polyethylene glycol in ethanol to prepare a drug-loaded layer solution with a drug concentration of 50 mg / mL, and spray the drug-loaded layer solution on the surface...
Embodiment 2
[0087] Same as Example 1, get 5 balloon catheters of 3.0mm*20mm (diameter*long), the material of the balloon of each balloon catheter is Pebax, and each balloon catheter is processed as follows:
[0088] Step 1: Wipe the surface of the balloon with 75% ethanol and set aside.
[0089] Step 2: Use plasma cleaning technology to clean the debris on the surface of the balloon. The plasma cleaning time is 15 minutes; the plasma cleaning technology uses argon as an inert gas, the power is 100KHz, and the pressure in the working chamber is 0.3atm during cleaning.
[0090] Step 3: Using dextran as the bottom layer material, spray a layer of dextran bottom layer with a molecular weight of 150K on the surface of the balloon, and the thickness of the bottom layer is 0.1 μm.
[0091] Step 4: Dissolve 500mg of paclitaxel and 5g of polyethylene glycol in ethanol to prepare a drug-loaded layer solution with a drug concentration of 50mg / mL, and spray the drug-loaded layer solution on the surfa...
PUM
Property | Measurement | Unit |
---|---|---|
Thickness | aaaaa | aaaaa |
Thickness | aaaaa | aaaaa |
Concentration | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com