Method for gradient separation and comprehensive recovery of gold concentrate containing carbon and arsenic
A technology for gold concentrate and carbon concentrate, which is applied to the improvement of process efficiency, photographic technology, instruments, etc., can solve the problems of decarburization, poor dearsenic boiling effect, and gold leaching rate from re-wrapping of gold particles, and achieves good results. Environmental benefits, friendly operation environment, simple process and technical conditions
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0027] 1) First-stage pre-flotation decarburization: mix the carbon-containing arsenic-containing gold concentrate with the two-stage roasting cyanide tailings, the mass ratio is 1:0.1, adjust the pulp concentration to 10%, adjust the pH to 9 with lime, and use the amount of sodium sulfite 500g / t, the amount of kerosene is 50g / t, after stirring for 10 minutes, add 2# oil 50g / t, stirring for 3 minutes, flotation time 10 minutes, using the first roughing, second sweeping and three times fine flotation process, scraping The foam produced is carbon concentrate, and the main components of carbon concentrate are 10% carbon, 50g / t gold, 300g / t silver, 3% sulfur, 5% lead, 3% copper, and 0.30% arsenic; The product in the tank is carbon beneficiation tailings, containing 0.2% carbon, 20g / t gold, 10g / t silver, 0.1% lead, 0.1% copper, 20% sulfur and 3% arsenic;
[0028] 2) Gold and silver extraction by high-concentration cyanide leaching of carbon concentrate: put the carbon concentrate i...
Embodiment 2
[0034] 1) First-stage pre-flotation decarburization: mix the carbon-containing arsenic-containing gold concentrate with the two-stage roasting cyanide tailings, the mass ratio is 1:0.3, adjust the pulp concentration to 15%, use lime to adjust the pH to 10, and the amount of sodium sulfite 1250g / t, kerosene dosage 175g / t, after stirring for 20 minutes, add 2# oil 125g / t, stirring for 4 minutes, flotation time of 25 minutes, using one roughing, two sweeping, three fine flotation process, scraping The froth is carbon concentrate, and the main components of carbon concentrate are 25% carbon, 125g / t gold, 450g / t silver, 5.5% sulfur, 6.5% lead, 4% copper, and 0.65% arsenic; The product in the tank is carbon beneficiation tailings, containing 0.3% carbon, 35g / t gold, 20g / t silver, 0.25% lead, 0.2% copper, 30% sulfur and 9% arsenic;
[0035] 2) Gold and silver extraction by high-concentration cyanidation leaching of carbon concentrate: put the carbon concentrate described in step 1) i...
Embodiment 3
[0041] 1) First-stage pre-flotation decarburization: mix the carbon-containing arsenic-containing gold concentrate with the two-stage roasting cyanide tailings, the mass ratio is 1:0.5, adjust the pulp concentration to 19%, use lime to adjust the pH to 11, and the amount of sodium sulfite 2000g / t, kerosene dosage 300g / t, after stirring for 30 minutes, add 2# oil 200g / t, stirring for 5 minutes, flotation time 40 minutes, using one roughing, two sweeping, three fine flotation processes, scraping The foam is carbon concentrate, and the main components of carbon concentrate are 40% carbon, 200g / t gold, 600g / t silver, 8% sulfur, 8% lead, 5% copper, and 1.00% arsenic. Carry out the next step of processing; the product in the tank is carbon tailings, containing 0.4% carbon, 50g / t gold, 30g / t silver, 0.4% lead, 0.3% copper, 40% sulfur, and 15% arsenic .
[0042] 2) Gold and silver extraction by high-concentration cyanide leaching of carbon concentrate: put the carbon concentrate desc...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com