Magnetic dextrin microspheres, preparation method and application in determination of residual quantity of chlorpyrifos in oyster mushrooms
A subtle and magnetic technology, applied in the field of detection of plant pesticide residues, can solve the problems of physical injury of test personnel, consumption of large organic solvents, cumbersome operation steps, etc., and achieve high accuracy, low solvent toxicity, and high enrichment multiples.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0058] A preparation method of magnetic dextrin microspheres, comprising the following steps:
[0059] S1, preparation of water phase:
[0060] Accurately weigh 4g of dextrin and 0.6g of NaOH into a 250mL conical flask, add 200mL of distilled water, and gelatinize at 85°C for 30min;
[0061] S2, preparation of oil phase:
[0062] Accurately weigh 6.6g of Span 60, 13.2g of Tween 80, and 100mL of n-hexane in a 250mL Erlenmeyer flask, and dissolve in a 50°C water bath, then add 0.01g of sodium trimetaphosphate and 0.01g of ferric iron tetroxide Powder, 18mL n-pentanol, mixed evenly to obtain the oil phase;
[0063] S3, preparation of magnetic nano-dextrin microspheres:
[0064] Add the water phase to the oil phase drop by drop and keep stirring. After the water and oil phases are mixed, stir with a high-speed homogenizer for 10 minutes, then place them in a water bath at 60°C for 3 hours, then break the emulsion at 85°C for 30 minutes, and remove the upper layer The oil phase...
Embodiment 2
[0074] A preparation method of magnetic dextrin microspheres, comprising the following steps:
[0075] S1, preparation of water phase:
[0076] Accurately weigh 4g of dextrin and 0.4g of NaOH into a 250mL Erlenmeyer flask, add 180mL of distilled water, and gelatinize at 80°C for 33min;
[0077] S2, preparation of oil phase:
[0078] Accurately weigh 6.6g of Span 60, 0.6g of Tween 80, and 80mL of n-hexane in a 250mL Erlenmeyer flask, dissolve them in a 45°C water bath, then add 0.03g of sodium trimetaphosphate and 0.02g of ferric oxide Powder, 20mL n-pentanol, mix well to get the oil phase;
[0079] S3, preparation of magnetic nano-dextrin microspheres:
[0080] Add the water phase to the oil phase drop by drop and keep stirring. After the water and oil phases are mixed, stir with a high-speed homogenizer for 10 minutes, then place them in a water bath at 55°C for 3.5 hours, then break the emulsion at 80°C for 30 minutes, and remove the upper layer The oil phase was alterna...
Embodiment 3
[0090] A preparation method of magnetic dextrin microspheres, comprising the following steps:
[0091] S1, preparation of water phase:
[0092] Accurately weigh 4g of dextrin and 0.8g of NaOH into a 250mL conical flask, add 200mL of distilled water, and gelatinize at 90°C for 30min;
[0093] S2, preparation of oil phase:
[0094] Accurately weigh 6.6g of Span 60, 9.9g of Tween 80, and 100mL of n-hexane in a 250mL Erlenmeyer flask, and dissolve in a 55°C water bath, then add 0.02g of sodium trimetaphosphate and 0.015g of ferric iron tetroxide Powder, 15mL n-pentanol, mix well to get the oil phase;
[0095] S3, preparation of magnetic nano-dextrin microspheres:
[0096] Add the water phase to the oil phase drop by drop and keep stirring. After the water and oil phases are mixed, stir with a high-speed homogenizer for 10 minutes, then place them in a 65°C water bath for 3 hours, then break the emulsion at 90°C for 30 minutes, and remove the upper layer The oil phase was washe...
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
particle diameter | aaaaa | aaaaa |
recovery rate | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com