Oxidized sodium alginate modified natamycin eye drops and preparation method thereof
A technology for oxidizing sodium alginate and natamycin, which is applied in the field of medical materials, can solve the problems of low degradation rate and achieve the effects of easy storage, low cost, and improved water solubility and permeability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0027] This example relates to oxidized sodium alginate modified natamycin eye drops, 1mL sterile deionized water contains 0.5-1.5mg oxidized sodium alginate-natamycin lyophilized powder, the specific preparation process is as follows :
[0028] The first step is to prepare oxidized sodium alginate:
[0029] (1) Weigh 10g of sodium alginate with a precision electronic balance, add 200mL of sterilized deionized water, stir magnetically at room temperature for 3-10 hours to prepare a sodium alginate aqueous solution with a mass concentration of 0.05g / mL, and add 1-10g of high iodine Sodium alginate, after reacting in the dark for 3-9 hours, add 0.260-2.60mL of ethylene glycol, magnetically stir for 0.5 hours, stop the reaction, generate oxidized sodium alginate (OSA) mixture solution, add 400mL of absolute ethanol to precipitate out , and then use a circulating water vacuum pump to filter under reduced pressure to obtain a mixed product containing OSA.
[0030] (2) Dissolve th...
Embodiment 2
[0036] This embodiment relates to the preparation method of natamycin eye drops modified by oxidized sodium alginate, and its specific preparation process is as follows:
[0037] The first step is to prepare oxidized sodium alginate:
[0038] Weigh 10g of sodium alginate with a precision electronic balance, add 200mL of sterilized deionized water, stir magnetically at room temperature for 6 hours to prepare a sodium alginate aqueous solution with a mass concentration of 0.05g / mL, add 5g of sodium periodate, and react in the dark for 6 hours Finally, add 1.430mL of ethylene glycol, magnetically stir for 0.5 hours, terminate the reaction, generate oxidized sodium alginate (OSA) mixture solution, add 400mL of absolute ethanol to precipitate the precipitate, and then use a circulating water vacuum pump to filter under reduced pressure to obtain Mixed product containing OSA.
[0039] The mixed product containing OSA was dissolved in sterilized deionized water, and then dialyzed in...
Embodiment 3
[0044] This embodiment relates to the preparation method of oxidized sodium alginate modified natamycin eye drops, and its specific preparation process is as follows: the first step, prepare oxidized sodium alginate:
[0045] (1) Weigh 10 g of sodium alginate with a precision electronic balance, add 200 mL of sterilized deionized water, stir magnetically at room temperature for 3 hours to prepare an aqueous sodium alginate solution with a mass concentration of 0.05 g / mL, add 1 g of sodium periodate, and avoid After 3 hours of photoreaction, add 0.260mL of ethylene glycol, stir magnetically for 0.5 hours, stop the reaction, generate oxidized sodium alginate (OSA) mixture solution, add 400mL of absolute ethanol to precipitate the precipitate, and then use a circulating water vacuum pump to depressurize Suction filtration to obtain a mixed product containing OSA.
[0046] (2) Dissolve the mixed product containing OSA in sterilized deionized water, then dialyze in sterilized doubl...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com