A painting and pigment technology, applied in the direction of art paints and coatings, can solve the problems of easy moisture-proof softening of paint films, short holding time of paintings, fading and other problems, and achieve the advantages of speeding up film forming time, improving stability and improving fineness. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0019] A paint paint resistant to dampness, comprising the following raw material components in parts by weight: 60 parts of acrylic emulsion, 5 parts of diatomaceous earth, 10 parts of talcum powder, 8 parts of toner, 8 parts of vegetable gum, 5 parts of hydroxyethyl cellulose 8 parts, moisturizing agent 8 parts, dispersant 0.3 parts, film former 3 parts, preservative 0.03 parts, water 12 parts.
[0020] A kind of preparation method of the anti-humidity painting pigment, comprises the steps:
[0021] (1) Weigh the diatomite, talcum powder and toner of the formula and place them in a high mixer for mixing. After the mixing is completed, place them in a ball mill for the first grinding. The grinding time is 2 hours to obtain the mixture A;
[0022] (2) Add water capable of wetting the mixture A in step (1), and grind it for the second time in a ball mill for 1 hour to obtain mixture B;
[0023] (3) Add the dispersant, film-forming agent, humectant and the remaining amount of w...
Embodiment 2
[0027] A paint paint resistant to dampness, comprising the following raw material components in parts by weight: 50 parts of acrylic acid emulsion, 8 parts of diatomaceous earth, 8 parts of talcum powder, 10 parts of toner, 5 parts of vegetable glue, and 8 parts of carboxymethyl cellulose 6 parts, 6 parts of humectant, 0.4 part of dispersant, 8 parts of film former, 0.05 part of preservative, 15 parts of water.
[0028] A kind of preparation method of the anti-humidity painting pigment, comprises the steps:
[0029] (1) Weigh the diatomite, talcum powder and toner of the formula amount and place them in a high-mixer for mixing. After the mixing is completed, place them in a ball mill for the first grinding. The grinding time is 3 hours to obtain the mixture A;
[0030] (2) Add water capable of wetting the mixture A in step (1), and grind it for the second time in a ball mill for 2 hours to obtain mixture B;
[0031] (3) Add the dispersant, film-forming agent, humectant and th...
Embodiment 3
[0035] A paint paint resistant to dampness, comprising the following raw material components in parts by weight: 55 parts of acrylic emulsion, 10 parts of diatomaceous earth, 5 parts of talcum powder, 12 parts of toner, 10 parts of vegetable gum, 3 parts of hydroxyethyl cellulose 3 parts of carboxymethyl cellulose, 5 parts of humectant, 0.5 part of dispersant, 5 parts of film former, 0.06 part of preservative, 10 parts of water.
[0036] A kind of preparation method of the anti-humidity painting pigment, comprises the steps:
[0037] (1) Weigh the diatomite, talcum powder and toner of the formula and place them in a high mixer for mixing. After the mixing is completed, place them in a ball mill for the first grinding. The grinding time is 2 hours to obtain the mixture A;
[0038] (2) Add water capable of wetting the mixture A in step (1), and grind it for the second time in a ball mill for 2 hours to obtain mixture B;
[0039] (3) Add the dispersant, film-forming agent, humec...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com