A technology for lithium-sulfur batteries and positive electrode materials, applied in battery electrodes, lithium batteries, non-aqueous electrolyte batteries, etc., can solve the problems of unsatisfactory capacity, poor battery cycle performance, poor conductivity, etc., and achieve the suppression of shuttle effect, strong chemical adsorption, The effect of increasing capacity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
specific Embodiment approach 1
[0017] Embodiment 1: This embodiment describes a lithium-sulfur battery positive electrode material, the positive electrode material includes activated carbon, carbon black, transition metal and sulfur, and the mass ratio of activated carbon, carbon black, transition metal and sulfur is 10~ 30: 1~10: 1~10: 60~80.
specific Embodiment approach 2
[0018] Specific embodiment two: a kind of positive electrode material of lithium-sulfur battery described in specific embodiment one, the specific surface area of described activated carbon is 1000~4000 m 2 / g; The specific surface area of the carbon black is 600~3000 m 2 / g; the transition metal is Ti, V, Cr, Mn, Fe, Co, Ni, Cu, Zn, Zr, Nb, Mo, Ru, Rh, Pd, Ag, Pt, lanthanide or actinide metal; Said sulfur is sublimed sulfur.
specific Embodiment approach 3
[0019] Specific embodiment three: a preparation method of a lithium-sulfur battery positive electrode material described in specific embodiment one or two, the preparation method is as follows: active carbon, carbon black and transition metal are mixed and ground until the mixture can be completely Sieve, then mix with sulfur, grind so that the mixture can be completely sieved, add carbon disulfide to submerge the solid surface, let it stand at room temperature until the carbon disulfide is volatilized, remove the sulfur precipitated on the surface, 60~100 o C blast drying for 6~24h, grinding and sieving, 150~350 o C is placed in a closed container and heated for 1-24 h, ground and sieved to obtain the lithium-sulfur battery positive electrode material; the mesh size of the sieve used is 50-300 mesh; the grinding is manual grinding or mechanical ball milling.
PUM
Property | Measurement | Unit |
---|---|---|
specific surface area | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com