A liquid fuel and alcohol-based technology, applied in the direction of liquid carbon-containing fuel, fuel, fuel additives, etc., can solve the problems of unstable quality, low calorific value, volatile, etc., to improve mixing efficiency, reduce fuel consumption, and not easy to separate layer effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0021] An alcohol-based liquid fuel, made from the following raw materials in parts by weight: 60 parts of methanol, 10 parts of ethanol, 3 parts of methylcyclopentadiene trihydroxy manganese, 5 parts of acetone, 5 parts of isopropanol, dimethyl ether 0.2 parts, hydrogen peroxide 0.5 parts, potassium permanganate 0.3 parts, ferrocene 0.2 parts, corrosion inhibitor 0.5 parts, water 5 parts, stabilizer 5 parts, industrial flavor 1 part. Wherein corrosion inhibitor comprises methylene diphosphonic acid, ethyl acetate and hexamethylene tetramine that mass ratio is 3:2:5; Stabilizer is di-tert-butyl p-cresol and that mass ratio is 3:2 A mixture of linseed oil.
[0022] The preparation method of above-mentioned alcohol base liquid fuel comprises the following steps:
[0023] Step a: Add linseed oil into reaction kettle A, heat to 300°C, add di-tert-butyl-p-cresol after cooling, mix well, and make a stabilizer for later use;
Embodiment 2
[0027] An alcohol-based liquid fuel, made from the following raw materials in parts by weight: 80 parts of methanol, 15 parts of ethanol, 5 parts of methylcyclopentadiene trihydroxymanganese, 10 parts of acetone, 7 parts of isopropanol, dimethyl ether 0.4 parts, 3 parts of hydrogen peroxide, 1 part of potassium permanganate, 0.3 parts of ferrocene, 0.7 parts of corrosion inhibitor, 7 parts of water, 10 parts of stabilizer, 2 parts of industrial flavor. Wherein wherein corrosion inhibitor comprises methylene diphosphonic acid, ethyl acetate and hexamethylenetetramine that mass ratio is 3:2:5; Stabilizer is isobutylamine and linseed oil that mass ratio is 3:2 composition of the mixture.
[0028] The preparation method of above-mentioned alcohol base liquid fuel comprises the following steps:
[0029] Step a: add linseed oil into reaction kettle A, heat to 300°C, add isobutylamine after cooling and mix evenly to make a stabilizer for later use;
[0030] Step b: First, add metha...
Embodiment 3
[0034] An alcohol-based liquid fuel, made of the following raw materials in parts by weight: 90 parts of methanol, 20 parts of ethanol, 7 parts of methylcyclopentadiene trihydroxymanganese, 20 parts of acetone, 10 parts of isopropanol, dimethyl ether 0.6 parts, hydrogen peroxide 5 parts, potassium permanganate 1.5 parts, ferrocene 0.5 parts, corrosion inhibitor 0.8 parts, water 10 parts, stabilizer 15 parts, industrial flavor 3 parts. Wherein wherein the corrosion inhibitor comprises methylene diphosphonic acid, ethyl acetate and hexamethylenetetramine with a mass ratio of 3:2:5; the stabilizer is dibutyl hydroxytoluene and cottonseed with a mass ratio of 3:2 A mixture of oils.
[0035] The preparation method of above-mentioned alcohol base liquid fuel comprises the following steps:
[0036] Step a: add cottonseed oil into reaction kettle A, heat to 300°C, add dibutyl hydroxytoluene after cooling and mix evenly to make a stabilizer for later use;
[0037] Step b: First, add ...
PUM
Property | Measurement | Unit |
---|---|---|
Density | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com