A technology of pearlescent dyes and pearlescent pigments, which is applied in the direction of paper, pigmented coating, pigment/opacifier addition, etc. It can solve the problems of unsatisfactory paper decoration effect, unsatisfactory matching and proportioning, and affecting the smoothness of paper. , to achieve the effect of rich color expression, good decorative effect and excellent color fidelity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0024] In this example, the pearlescent dye for papermaking is made from the following percentages of raw materials: 25% modified kaolin, 5% citric acid, 5% neopentyl glycol, 10% pearlescent pigment, 1% thickener, and 1% dispersant , the balance is deionized water;
[0025] Among them, the modification method of the modified kaolin is: take 1g of silane coupling agent and mix it with 25mL ethanol, then use acetic acid aqueous solution to adjust the pH value to 5.5-7 to obtain a hydrolyzed silane coupling agent solution, add 8g of kaolin to In the hydrolyzed silane coupling agent solution, heated to 60°C for 2 hours, filtered, washed, dried, and ground through a 300-mesh sieve to obtain modified kaolin;
[0026] The thickener is methyl methacrylate; the dispersant is sodium lignosulfonate; the pearlescent pigment is 100# pearlescent gold;
[0027] The preparation method of pearlescent dye for papermaking of the present embodiment comprises the following steps:
[0028] S1, we...
Embodiment 2
[0033] In this example, the pearlescent dye for papermaking is made from the following percentages of raw materials: 38% modified kaolin, 9% citric acid, 12% neopentyl glycol, 18% pearlescent pigment, 2% thickener, and 3% dispersant , the balance is deionized water;
[0034] Among them, the modification method of the modified kaolin is: take 1g of silane coupling agent and mix it with 25mL ethanol, then use acetic acid aqueous solution to adjust the pH value to 5.5-7 to obtain a hydrolyzed silane coupling agent solution, add 8g of kaolin to In the hydrolyzed silane coupling agent solution, heated to 70°C for 3 hours, filtered, washed, dried, and ground through a 300-400 mesh sieve to obtain modified kaolin;
[0035] The thickener is isooctyl methacrylate; the dispersant is methyl methacrylate-maleic anhydride copolymer; the pearlescent pigment is 100# pearlescent gold;
[0036] The preparation method of pearlescent dye for papermaking of the present embodiment comprises the f...
Embodiment 3
[0042] In this example, the pearlescent dye for papermaking is made from the following percentages of raw materials: 32% modified kaolin, 7% citric acid, 8% neopentyl glycol, 14% pearlescent pigment, 1.5% thickener, and 2% dispersant , the balance is deionized water;
[0043] Among them, the modification method of the modified kaolin is: take 1g of silane coupling agent and mix it with 25mL ethanol, then use acetic acid aqueous solution to adjust the pH value to 5.5-7 to obtain a hydrolyzed silane coupling agent solution, add 8g of kaolin to In the hydrolyzed silane coupling agent solution, heated to 65°C for 2.5 hours, filtered, washed, dried, and ground through a 360-mesh sieve to obtain modified kaolin;
[0044] The thickener is ethyl acrylate; the dispersant is dispersant CNF; the pearlescent pigment is 100# pearlescent gold;
[0045] The preparation method of pearlescent dye for papermaking of the present embodiment comprises the following steps:
[0046] S1, weighing e...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com