A clothing and fabric technology, which is applied in the field of coating and preparation of firefighting clothing fabrics, can solve the problems of reducing the layers of firefighting clothing fabrics, difficult operation, and bulky firefighting clothing, so as to improve wear resistance, impact resistance and tensile strength Good tensile strength and waterproof effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0035] This embodiment relates to a coating used for fire-fighting clothing fabrics, including the following raw materials in parts by weight: 20 parts of styrene-acrylic emulsion, 15 parts of epoxy emulsion, 10 parts of polyurethane emulsion, 7 parts of terpene resin, 6 parts of acrylic resin, modified 6 parts of talcum powder, 4 parts of attapulgite, 3 parts of polyvinylidene fluoride, 4 parts of hollow floating beads, 2 parts of polyvinyl alcohol, 4 parts of modified nano-expanded vermiculite, 2 parts of ethyl cellulose, and 3 parts of reinforcing fiber 2 parts, 2 parts of calcium stearate, 2 parts of thickener, 3 parts of flame retardant, 1 part of nano-silver ion fungicide.
[0036] Wherein, the preparation method of the modified nano expanded vermiculite is as follows:
[0037] Soak the expanded vermiculite in the sodium alginate sol prepared in advance, and adopt the vacuum impregnation and adsorption process to make the nano-sodium alginate sol suck into the cavity of ...
Embodiment 2
[0050] This embodiment relates to a coating used for fire-fighting clothing fabrics, including the following raw materials in parts by weight: 30 parts of styrene-acrylic emulsion, 25 parts of epoxy emulsion, 20 parts of polyurethane emulsion, 11 parts of terpene resin, 14 parts of acrylic resin, modified 9 parts of talcum powder, 7 parts of attapulgite, 6 parts of polyvinylidene fluoride, 8 parts of hollow floating beads, 5 parts of polyvinyl alcohol, 9 parts of modified nano-expanded vermiculite, 3 parts of ethyl cellulose, and 6 parts of reinforcing fiber 4 parts, 4 parts of calcium stearate, 3 parts of thickener, 4 parts of flame retardant, 2 parts of nano-silver ion bactericide.
[0051] Wherein, the preparation method of the modified nano expanded vermiculite is as follows:
[0052] Soak the expanded vermiculite in the sodium alginate sol prepared in advance, and adopt the vacuum impregnation and adsorption process to make the nano-sodium alginate sol suck into the cavit...
Embodiment 3
[0065] This embodiment relates to a coating used for fire-fighting clothing fabrics, including the following raw materials in parts by weight: 23 parts of styrene-acrylic emulsion, 17 parts of epoxy emulsion, 13 parts of polyurethane emulsion, 8 parts of terpene resin, 7 parts of acrylic resin, modified 7 parts of talcum powder, 5 parts of attapulgite, 4 parts of polyvinylidene fluoride, 5 parts of hollow floating beads, 3 parts of polyvinyl alcohol, 5 parts of modified nano-expanded vermiculite, 2.3 parts of ethyl cellulose, and 4 parts of reinforcing fiber 2.8 parts, 2.8 parts of calcium stearate, 2.4 parts of thickener, 3.2 parts of flame retardant, 1.3 parts of nano-silver ion fungicide.
[0066] Wherein, the preparation method of the modified nano expanded vermiculite is as follows:
[0067] Soak the expanded vermiculite in the sodium alginate sol prepared in advance, and adopt the vacuum impregnation and adsorption process to make the nano-sodium alginate sol suck into t...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com