Method for preparing air layer fabric with good warming effect
A production method and air layer technology, which are applied in the direction of fabric surface trimming, spraying/jetting textile material treatment, roughening, etc., can solve the problems of poor thermal insulation effect, easy to absorb dust, easy to generate static electricity, etc., to prevent heat loss, Good thermal insulation effect and gloss-enhancing effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0024] A method for manufacturing an air layer fabric with a good heat-retaining effect, the specific steps of the method are as follows:
[0025] Step 1: First use conductive fiber yarn, 32s cotton, 75D / 36F low stretch yarn and 60 / 40 cotton polyester 34s as raw materials, and use a 38-inch 18-knitting double-sided large circular machine to weave the face and lining.
[0026] Step 2: Perform anti-wrinkle treatment on the face and lining prepared in step 1, rinse and dry after the anti-wrinkle treatment.
[0027] Step 3: Stretch the face and lining prepared in step 2, put them into a concentrated caustic soda solution and soak for 10-20 minutes, then take out the face and lining, wash them in the stretched state, and then dry them.
[0028] Step 4: Connect the face and lining obtained in step 3 with stretched textured yarns to obtain a pre-fabric, and at the same time form an air interlayer between the face and the lining.
[0029] Step 5: Fill the air interlayer of the pre-fa...
Embodiment 2
[0039] A method for manufacturing an air layer fabric with a good heat-retaining effect, the specific steps of the method are as follows:
[0040] Step 1: First use conductive fiber yarn, 32s cotton, 75D / 36F low stretch yarn and 60 / 40 cotton polyester 34s as raw materials, and use a 38-inch 18-knitting double-sided large circular machine to weave the face and lining.
[0041] Step 2: Perform anti-wrinkle treatment on the face and lining prepared in step 1, rinse and dry after the anti-wrinkle treatment.
[0042] Step 3: Stretch the face and lining prepared in step 2, put them into a concentrated caustic soda solution and soak for 10-20 minutes, then take out the face and lining, wash them in the stretched state, and then dry them.
[0043] Step 4: Connect the face and lining obtained in step 3 with stretched textured yarns to obtain a pre-fabric, and at the same time form an air interlayer between the face and the lining.
[0044] Step 5: Fill the air interlayer of the pre-fa...
Embodiment 3
[0054] A method for manufacturing an air layer fabric with a good heat-retaining effect, the specific steps of the method are as follows:
[0055] Step 1: First use conductive fiber yarn, 32s cotton, 75D / 36F low stretch yarn and 60 / 40 cotton polyester 34s as raw materials, and use a 38-inch 18-knitting double-sided large circular machine to weave the face and lining.
[0056] Step 2: Perform anti-wrinkle treatment on the face and lining prepared in step 1, rinse and dry after the anti-wrinkle treatment.
[0057] Step 3: Stretch the face and lining prepared in step 2, put them into a concentrated caustic soda solution and soak for 10-20 minutes, then take out the face and lining, wash them in the stretched state, and then dry them.
[0058] Step 4: Connect the face and lining obtained in step 3 with stretched textured yarns to obtain a pre-fabric, and at the same time form an air interlayer between the face and the lining.
[0059] Step 5: Fill the air interlayer of the pre-fa...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com