[0022] Weigh the raw materials of the following weight proportions:
[0023] Liquid polyisoprene rubber: 55g
[0024] Sodium carboxymethylcellulose: 20g
[0025] Karaya gum: 10g
[0026] White carbon black: 2g
[0027] Inorganic clay: 6g
[0028] Glycerin: 2g
[0029] 1. 2-propanediol: 4g
[0030] 1. 3-Butanediol: 1g
[0031] Mineral oil: 4g.
[0032] According to the above ratio, add weighed liquid polyisoprene rubber, glycerin, mineral oil, 1.2-propylene glycol, 1.3-butanediol into the internal mixer, stir for half an hour until completely uniform, add white carbon black and For inorganic clay, stir for 1 hour until uniform; finally add sodium carboxymethyl cellulose and karaya gum, and continue stirring for 1 hour until uniform.
Embodiment 2
[0034] Weigh the raw materials of the following weight proportions:
[0035] Liquid polyisoprene rubber: 40g
[0036] Sodium carboxymethylcellulose: 40g
[0037] Karaya gum: 5g
[0038] White carbon black: 6g
[0039] Inorganic clay: 2g
[0040] Glycerin: 4g
[0041] 1. 2-Propanediol: 1g
[0042] 1. 3-Butanediol: 4g
[0043] Mineral oil: 1 g.
[0044] According to the above ratio, add weighed liquid polyisoprene rubber, glycerin, mineral oil, 1.2-propylene glycol, 1.3-butanediol into the internal mixer, stir for half an hour until completely uniform, add white carbon black and For inorganic clay, stir for 1 hour until uniform; finally add sodium carboxymethyl cellulose and karaya gum, and continue stirring for 1 hour until uniform.
Embodiment 3
[0046] Weigh the raw materials of the following weight proportions:
[0047] Liquid polyisoprene rubber: 50g
[0048] Sodium carboxymethylcellulose: 25g
[0049] Karaya gum: 6g
[0050] White carbon black: 5g
[0051] Inorganic clay: 4g
[0052] Glycerin: 3g
[0053] 1. 2-propanediol: 2g
[0054] 1. 3-Butanediol: 2g
[0055] Mineral oil: 2g.
[0056] According to the above ratio, add weighed liquid polyisoprene rubber, glycerin, mineral oil, 1.2-propylene glycol, 1.3-butanediol into the internal mixer, stir for half an hour until completely uniform, add white carbon black and For inorganic clay, stir for 1 hour until uniform; finally add sodium carboxymethyl cellulose and karaya gum, and continue stirring for 1 hour until uniform.
PUM
Property | Measurement | Unit |
---|---|---|
Sheet diameter | aaaaa | aaaaa |
Thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com