Embodiment 1
[0030] 1) Place the two ends of the hollow fiber in two disconnected containers respectively, submerge the first end of the hollow fiber in the silver nitrate mixed solution, leave the second end of the hollow fiber empty in the container, and make the second end A height difference H is formed between the first end and the first end, and the height difference H is 1 cm. The mixed solution of silver nitrate includes ammonia water and AgNO with a volume ratio of 9:7:4. 3 solution and glucose solution, the concentration of ammonia water is 5% by mass, AgNO 3 The concentration of the solution is 10% by mass, and the concentration of glucose is 10% by mass;
[0031] 2) and blow air vertically at the end of the second end of the hollow fiber with a flow velocity of 50m / s, so that the mixed solution of silver nitrate passes through the hollow fiber, and is attached to the inner wall of the hollow fiber, so that the inner wall is attached with the mixed solution of silver nitrate. f...
Embodiment 2
[0038] 1) Place the two ends of the hollow fiber in two disconnected containers respectively, submerge the first end of the hollow fiber in the silver nitrate mixed solution, leave the second end of the hollow fiber empty in the container, and make the second end A height difference is formed between the first end and the first end, and the height difference is 5cm. The silver nitrate mixed solution includes ammonia water, AgNO 3 solution and glucose solution, the concentration of ammonia water is 2% by mass, AgNO 3 The concentration of the solution is 4% by mass, and the concentration of glucose is 4% by mass;
[0039] 2) and blow air vertically at the end of the second end of the hollow fiber with a flow velocity of 10m / s, so that the mixed solution of silver nitrate passes through the hollow fiber, and is attached to the inner wall of the hollow fiber, so that the inner wall is attached with the mixed solution of silver nitrate. fiber;
[0040] 3) The hollow fiber with th...
Embodiment 3
[0042] 1) Place the two ends of the hollow fiber in two disconnected containers respectively, submerge the first end of the hollow fiber in the silver nitrate mixed solution, leave the second end of the hollow fiber empty in the container, and make the second end A height difference H is formed between the first end and the first end, and the height difference H is 10cm. The ammonia water and AgNO in the silver nitrate mixed solution3 solution and glucose solution, the concentration of ammonia water is 10% by mass, AgNO 3 The concentration of the solution is 2% by mass, and the concentration of glucose is 0.2% by mass;
[0043] 2) and blow air vertically at the end of the second end of the hollow fiber with a flow velocity of 100m / s, so that the mixed solution of silver nitrate passes through the hollow fiber, and is attached to the inner wall of the hollow fiber, so that the inner wall is attached with the mixed solution of silver nitrate. fiber;
[0044] 3) The hollow fiber...
PUM
Property | Measurement | Unit |
---|---|---|
diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com