Method for preparing low-dielectric-constant low-temperature co-fired ceramic (LTCC) powder with sol-gel method
A technology of low-temperature co-fired ceramics and low dielectric constant, applied in the field of ceramic powder production, can solve the problems of destroying the ecological environment, unqualified quality, and reducing market competitiveness, etc., and achieve simple formula, low dielectric loss, and low softening point effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0024] The invention provides a technical solution: a method for preparing a low-dielectric constant low-temperature co-fired ceramic powder by using a sol-gel method, comprising the following steps:
[0025] Step 1: Materials: Take materials according to 5 moles of calcium carbonate, 18 moles of tetraethyl orthosilicate, 18 moles of ethanol, 60 moles of tributyl borate, and 60 moles of water;
[0026] Step 2: Preparation of low softening point CaO-B 2 o 3 -SiO 2 (hereinafter referred to as CBS) precursor powder:
[0027] First, add tetraethyl orthosilicate, ethanol and an appropriate amount of water into a container to form a uniform and transparent solution, and slowly drop tributyl borate into the solution to obtain a transparent solution 1;
[0028] Secondly, the obtained calcium carbonate was dissolved in dilute nitric acid to obtain a transparent solution 2;
[0029] Finally, place the transparent solution 1 on a stable heating operation table, slowly drop the transp...
Embodiment 2
[0032] A method for preparing a low-dielectric constant low-temperature co-fired ceramic powder by a sol-gel method, comprising the following steps:
[0033] Step 1: Materials: Take materials according to 5 moles of calcium carbonate, 18 moles of tetraethyl orthosilicate, 18 moles of ethanol, 60 moles of tributyl borate, and 60 moles of water;
[0034] Step 2: Preparation of low softening point CaO-B 2 o 3 -SiO 2 (hereinafter referred to as CBS) precursor powder:
[0035] First, add tetraethyl orthosilicate, ethanol and an appropriate amount of water into a container to form a uniform and transparent solution, and slowly drop tributyl borate into the solution to obtain a transparent solution 1;
[0036] Secondly, the obtained calcium carbonate was dissolved in dilute nitric acid to obtain a transparent solution 2;
[0037] Finally, place the transparent solution 1 on a stable heating operation table, slowly drop the transparent solution 2 into the transparent solution 1, s...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com