[0036] (3) Preparation of melamine resin prepolymer
[0037] Put 5-10 parts of melamine and 10-20 parts of 37% formaldehyde solution into a four-necked bottle in parts by weight, heat up to 60-80°C under stirring conditions, and add 0.1-1 part of triethanolamine after the melamine is completely dissolved, Adjust the pH to 7-10, and react for 10-30 minutes to obtain a transparent and viscous melamine resin prepolymer;
[0038] (4) Preparation of self-adhesive double-wall essence microcapsules
[0039] By weight, 10-30 parts of essence, 2-5 parts of methyl methacrylate, 2-5 parts of acrylonitrile, 1-3 parts of butyl acrylate, 1-3 parts of isooctyl acrylate, 0.2-0.5 parts of methyl Acrylic acid, 0.2-0.5 parts of hydroxyethyl acrylate, 0.1-0.3 parts of diacetone acrylamide, 0.1-0.3 parts of adipic acid dihydrazide, and 0.02-0.05 parts of azobisisobutyronitrile are placed in a beaker at a temperature of 30 Stir and mix at -50°C to form a homogeneous oil solution;
[0040]Mix the...
Embodiment 1
[0044] (1) Preparation of styrene-maleic anhydride copolymer powder
[0045] A, maleic anhydride and benzoyl peroxide are added to dissolve in the toluene of 90ml;
[0046] B. Dissolve styrene in 70ml-90ml toluene, heat to 80°C while stirring;
[0047] C. Mix dodecyl mercaptan with 30ml-50ml toluene, heat to 80°C while stirring;
[0048] D. When the solution obtained in step A is heated to ℃, while adding the solution obtained in step B dropwise, add the solution obtained in step C dropwise. After the dropwise addition, heat to 90 ℃ and keep it warm, and stir for 3 hours to obtain low molecular weight styrene-malay Anhydride polymer dispersion system;
[0049] E, suction filtration, 80 ℃ of vacuum dryings, obtain low molecular weight-maleic anhydride copolymer, and the number-average molecular weight of copolymer is 10000;
[0050] Described reaction system comprises two kinds of monomer maleic anhydride and styrene, initiator, solvent and polymerization inhibitor, the tota...
Embodiment 2
[0061] (1) Preparation of styrene-maleic anhydride copolymer powder
[0062] A, maleic anhydride and lauryl peroxide are added to dissolve in the chlorobenzene of 70ml;
[0063] B. Dissolve styrene in 70mlml chlorobenzene, heat to 65°C while stirring;
[0064] C. Mix propanethiol with 30mlml chlorobenzene, stir while heating to 65°C and keep warm;
[0065] D. When the solution obtained in step A is heated to 65°C, while adding the solution obtained in step B dropwise, add the solution obtained in step C dropwise. After the dropwise addition, heat to 75°C and keep it warm, and stir for 1.8 hours to obtain low molecular weight styrene- Maleic anhydride polymer dispersion system;
[0066] E, suction filtration, 60 ℃ of vacuum dryings, obtain low molecular weight-maleic anhydride copolymer, and the number-average molecular weight of copolymer is 5000;
[0067] Described reaction system comprises two kinds of monomer maleic anhydride and styrene, initiator, solvent and polymeriz...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com