A wood and mildew-proof technology, applied in the direction of wood treatment, wood impregnation, wood impregnation, etc., can solve the problems of environmental pollution, moth-eaten, harm to human health, etc., to improve economic income, reduce treatment traces, and inhibit mold and moth-eaten problems. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0023] A method for softening and preventing mildew of wood, comprising the following steps:
[0024] (1) Timber finishing: peel off the bark of the wood, cut it according to the required length and width, and get the wood blank;
[0025] (2) Wood acid soaking: put the wood blank in a boiled acetic acid solution with a volume fraction of 1.2%, and soak it at 75~80°C for 9 hours, which can promote the entry of water into the wood fiber, reduce the pH of the wood, and accelerate the softening of the wood fiber. Cool down to 30~35°C, ferment to get sour foam wood;
[0026] (3) Alkaline cleaning of wood: Put the acid-foamed wood in the treatment room, spray the edible alkali solution with a mass concentration of 1.6% evenly on the acid-foamed wood, spray repeatedly 5 times, neutralize the residual acetic acid in the wood, and carry out after spraying. Freezing and thawing can make the water change into crystal water repeatedly, increase the intercellular space of wood, improve th...
Embodiment 2
[0040] A method for softening and preventing mildew of wood, comprising the following steps:
[0041] (1) Timber finishing: peel off the bark of the wood, cut it according to the required length and width, and get the wood blank;
[0042] (2) Wood acid soaking: put the wood blank in a boiled acetic acid solution with a volume fraction of 1.3%, and soak it at 75~80°C for 9 hours, which can promote the entry of water into the wood fiber, reduce the pH of the wood, and accelerate the softening of the wood fiber. Cool down to 30~35°C, ferment to get sour foam wood;
[0043] (3) Alkaline cleaning of wood: Put the acid-foamed wood in the treatment room, spray the edible alkali solution with a mass concentration of 1.7% evenly on the acid-foamed wood, spray repeatedly 5 times, neutralize the residual acetic acid in the wood, and carry out after spraying. Freezing and thawing can make the water change into crystal water repeatedly, increase the intercellular space of wood, improve th...
Embodiment 3
[0057] A method for softening and preventing mildew of wood, comprising the following steps:
[0058] (1) Timber finishing: peel off the bark of the wood, cut it according to the required length and width, and get the wood blank;
[0059] (2) Wood acid soaking: put the wood blank in a boiled acetic acid solution with a volume fraction of 1.4%, and soak it at 75~80°C for 10 hours, which can promote the entry of water into the wood fiber, reduce the pH of the wood, and accelerate the softening of the wood fiber. Cool down to 30~35°C, ferment to get sour foam wood;
[0060] (3) Alkaline cleaning of wood: put the acid-foamed wood in the treatment room, spray the edible alkali solution with a mass concentration of 1.8% evenly on the acid-foamed wood, spray repeatedly 5 times, neutralize the residual acetic acid in the wood, and carry out after spraying. Freezing and thawing can make the water change into crystal water repeatedly, increase the intercellular space of wood, improve t...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com