Thermoplastic elastomer and preparation method therefor
A thermoplastic elastomer and base oil technology, applied in the field of thermoplastic elastomers, can solve problems such as sole breakage, easy slipping, and low wear resistance, and achieve the effects of reduced density, good skid resistance, and increased heat resistance temperature
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0018] The present invention also provides a preparation method of thermoplastic elastomer, which comprises the following parts by weight: 33-40 parts of base oil, 35-45 parts of calcium powder of 1000-1250 mesh, 15 parts of styrene-butadiene-styrene block copolymer ~20 parts, 15~20 parts of styrene-ethylene-butylene-styrene block copolymer, 1-3 parts of cyclohexane and 1-3 parts of polyurethane are mixed, and heated at 150-175 degrees Celsius for 5-7 hours , that is, a thermoplastic elastomer.
[0019] As can be seen from the above description, the beneficial effects of the present invention are: adding cyclohexane and polyurethane in a certain proportion to the original formula, and heating at 150-175 degrees centigrade for 5-7 hours, the Acron wear volume of the obtained sole is lower than 0.6cm 3 / 1.61km, the wear resistance is close to the requirements of automobile tires; polyurethane increases the surface roughness of thermoplastic elastomers, making it better in skid ...
Embodiment 1
[0024] A preparation method of a thermoplastic elastomer, the following parts by weight of base oil (CNOOC II hydrogenated base oil 60N) 36 parts, 1000 ~ 1250 mesh calcium powder 40 parts, styrene-butadiene-styrene block copolymerization Compound (Maoming Petrochemical thermoplastic styrene-butadiene rubber SBS675) 17 parts, styrene-ethylene-butylene-styrene block copolymer (Baling Petrochemical thermoplastic rubber SEBSYH-503) 17 parts, cyclohexane 2 parts and polyurethane 2 parts mixed , and heated at 162 degrees Celsius for 6 hours, and stirred at a speed of 350 r / min while heating to obtain a thermoplastic elastomer.
[0025] After testing, 80 pairs of shoe soles can be made per 5kg of thermoplastic elastomer, and the Akron wear volume of the shoe soles is 0.50cm 3 / 1.61km, light weight, non-slip and good wear resistance.
Embodiment 2
[0027] A preparation method of a thermoplastic elastomer, the following parts by weight of base oil (CNOOC II hydrogenated base oil 150N) 33 parts, 1000 ~ 1250 mesh calcium powder 35 parts, styrene-butadiene-styrene block copolymerization Compound (Maoming Petrochemical thermoplastic styrene-butadiene rubber SBS675) 15 parts, styrene-ethylene-butylene-styrene block copolymer (Baling Petrochemical thermoplastic rubber SEBSYH-503) 15 parts, cyclohexane 1 part and polyurethane 1 part , and heated at 150 degrees Celsius for 5 hours, and stirred at a speed of 300 r / min while heating to obtain a thermoplastic elastomer.
[0028] After testing, 70 pairs of soles can be made for every 5kg of thermoplastic elastomer, and the Akron wear volume of the obtained soles is 0.53cm 3 / 1.61km, light weight, non-slip and good wear resistance.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com