Technology for manufacturing pencil leads by waste plants
A technology of discarded plants and pencil cores, which is applied in the field of manufacturing pencil cores, can solve the problems of secondary pollution of water bodies, etc., and achieve the effects of rational utilization, no slag dropping, and saving straw incineration
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0026] A pencil lead made of waste plants, characterized in that it includes plant raw materials, scale stone mills and binders, and the components by weight ratio are: 200 parts of plant raw materials, 60 parts of scale stone mills, and 30 parts of binders , 240 parts of water.
[0027] A kind of technology that utilizes waste plant to manufacture pencil lead, it is characterized in that: comprise the following steps:
[0028] (1) Pretreat the plant raw material, heat it in a sealed oxygen-insulated environment to obtain ash, the heating temperature is 400°C, and the time is 5 hours;
[0029] (2) Grinding the scale stone mill into fine powder, adding water after weighing with ash and binder, mixing under normal temperature conditions to obtain a mixture;
[0030] (3) The mixture is kneaded and rolled in the equipment, and then crushed and extruded with rods;
[0031] (4) The extruded bar is core-pressed and core-cut, and then rotated and dried. After drying, it enters the b...
Embodiment 2
[0039] A pencil lead made of waste plants, characterized in that it includes plant raw materials, scale stone mills and binders, and the components by weight ratio are: 170 parts of plant raw materials, 50 parts of scale stone mills, and 20 parts of binders , 220 parts of water.
[0040] A kind of technology that utilizes waste plant to manufacture pencil lead, it is characterized in that: comprise the following steps:
[0041] (1) Pretreat the plant raw material, heat it in a sealed oxygen-insulated environment to obtain ash, the heating temperature is 400°C, and the time is 5 hours;
[0042] (2) Grinding the scale stone mill into fine powder, adding water after weighing with ash and binder, mixing under normal temperature conditions to obtain a mixture;
[0043] (3) The mixture is kneaded and rolled in the equipment, and then crushed and extruded with rods;
[0044] (4) The extruded bar is core-pressed and core-cut, and then rotated and dried. After drying, it enters the b...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com