Preparation method for novel rare-earth fluorescent gel adopting PVA as main body and application thereof
A rare earth and gel technology, applied in the field of rare earth polymer composite luminescent materials, achieves the effects of good chemical stability, improved fluorescence intensity and good biocompatibility
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0041] Example 1: Rare Earth Terbium Complex Tb(ACAC) 3 2H 2 The preparation method of O comprises the steps:
[0042] First weigh 3.03g (30mmol) acetylacetone and add it into a 100ml three-necked flask, then add 50ml of THF to dissolve it, and the water bath is heated to 65 , add dropwise 2.83g of TbCl that has been dissolved in 20ml of absolute ethanol 3 ·6H 2 O (10mmol), 65 Continue to react for 4h, add an appropriate amount of NaOH aqueous solution to adjust the pH value to neutrality during the reaction, and remove the solvent by rotary distillation after the reaction is completed. The solid product obtained is rinsed with an appropriate amount of distilled water and dehydrated alcohol for about three times respectively, and finally 4g light yellow product ( Tb(ACAC) 3 2H 2 O), its productive rate 80.8%.
[0043] From figure 2 As can be seen in the terbium complex Tb(ACAC) 3 2H 2 The main absorption peak of O is at 293nm. The peak here mainly reflects the ...
Embodiment 6
[0047] Embodiment 6: The preparation method of fluorescent gel, adopts the rare earth terbium complex Tb(ACAC) prepared in embodiment 1-5 3 2H 2 O as a luminescent molecule, and then the rare earth terbium complex Tb(ACAC) 3 2H 2 O was introduced into the PVA matrix to form a fluorescent gel under the action of a crosslinker.
[0048] Weigh 0.5g PVA, 0.05g boric acid (dissolve with appropriate amount of deionized water after weighing), 0.007g NaOH (dissolve with appropriate amount of deionized water after weighing), and 0.015g terbium complex (dissolve with appropriate amount of DMF). Then measure 4.5ml of deionized water in a 5ml round bottom flask, and the water bath is heated to 90 Add the weighed polyvinyl alcohol and stir to dissolve. When the PVA is completely dissolved, add the boric acid solution. When the solution is evenly mixed, add the terbium complex solution (the mass ratio to PVA is 3%). After mixing evenly, pour the NaOH solution. After cooling, the PVA fl...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com