A multi-element alloy, a new type of technology, applied in heat treatment furnaces, heat treatment equipment, manufacturing tools, etc., can solve the problems of large throwing wear, poor impact resistance, etc., to reduce production costs and energy consumption, good mechanical properties, and impact resistance The effect of toughness and not easy to wear
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0024] In this embodiment, a new type of multi-element alloy grinding forging, its composition is by mass percentage:
[0025] C:2.2%; Si:1.0%; Mn:0.3%; Cr:10%; Re:0.15%; P:0.02%; S:0.05%; V:0.1%; Ti:0.2%; Al:0.06%; The balance is Fe.
[0026] The size of the new multi-element alloy grinding forging is Ф40mm×50mm, and the thickness of the sand-coated layer in the sand-coated metal mold process is 3mm.
Embodiment 2
[0028] In this embodiment, a new type of multi-element alloy grinding forging, its composition is by mass percentage:
[0029] C: 2.5%; Si: 0.6%; Mn: 0.5%; Cr: 16%; Re: 0.1%; P: 0.03%; The balance is Fe.
[0030] The size of the new multi-element alloy grinding forging is Ф50mm×60mm, and the thickness of the sand-coated layer in the sand-coated metal mold process is 3.5mm.
Embodiment 3
[0032] In this embodiment, a new type of multi-element alloy grinding forging, its composition is by mass percentage:
[0033] C: 2.8%; Si: 0.3%; Mn: 0.8%; Cr: 14%; Re: 0.08%; P: 0.05%; The balance is Fe.
[0034] The size of the new multi-element alloy grinding forging is Ф60mm×70mm, and the thickness of the sand-coated layer in the sand-coated metal mold process is 4mm.
[0035] Based on the multi-element alloy grinding and forging disclosed in the above-mentioned embodiments 1 to 3, the present invention proposes a heat treatment process for a novel multi-element alloy grinding and forging, which includes the following steps:
[0036] S1. Quenching process:
[0037] Put the semi-finished grinding forging into the heating furnace, heat up to 320-380°C, preferably 340-360°C, such as 345°C, 350°C, 355°C, holding time 80-120min, preferably 90-110°C, such as 95°C, 100°C, 105°C;
[0038] Heat up to 480-530°C, preferably 490-510°C, such as 495°C, 500°C, 505°C, holding time for...
PUM
Property | Measurement | Unit |
---|---|---|
thickness | aaaaa | aaaaa |
thickness | aaaaa | aaaaa |
thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com