Fluorite slag aerated brick and preparation method thereof
A technology of fluorite slag and aerated bricks, which is applied in the field of fluorite slag aerated bricks and their preparation, can solve problems such as land occupation and environmental pollution, and achieve the effects of protecting the environment, reducing bulk density and reducing energy consumption.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0025] Weigh the following raw materials in parts by weight: fluorite slag 20-30, sand 25-30, cement 5-10, modified nano-attapulgite 4-6, ceramsite 5-10, ceramic factory waste 5-10, light calcium Powder 5-10, lime 10-15, triethanolamine lime 0.1-0.3% by weight, gypsum 1-3, aluminum powder 0.02-0.08, oxidized paraffin wax soap 3-5% by aluminum powder weight, calcium bicarbonate 0.01 -0.02, volcanic rock 2-3, lignocellulose 1-2, water glass 0.3-0.5, sodium hexametaphosphate 1-2, borax 0.03-0.05, hydroxypropyl methylcellulose sodium 1-2, ultrafine polyethylene Alcohol 1-2,
[0026] Among them, the attapulgite is modified: first soak the attapulgite with 15-20% hydrochloric acid for 1-2 hours, let it stand, clarify, centrifuge, wash the solid with water until it is neutral, and after drying, add an amount equivalent to the weight of the solid 3-5% vinyltriethoxysilane is stirred evenly, dried and ground into nanopowder,
[0027] Process the above-mentioned substances that have b...
Embodiment 2
[0035] Weigh the following raw materials in parts by weight: fluorite slag 25, cement 56, modified nano-attapulgite 5, ceramsite 8, ceramic factory waste 6, light calcium powder 12, lime 14, 0.1-0.3% of the weight of triethanolamine lime , gypsum 2, aluminum powder 0.05, the amount of oxidized paraffin wax soap is 4% of the weight of aluminum powder, calcium bicarbonate 0.01, volcanic rock 3, lignocellulose 1.5, water glass 0.4, sodium hexametaphosphate 1, borax 0.04, hydroxypropyl Sodium methyl cellulose 2, superfine polyvinyl alcohol 1, wherein, modified attapulgite is obtained by following method: first soak sepiolite with 15% hydrochloric acid for 1-2 hours, let stand, clarify, centrifuge, and use for solid Wash with water until neutral, after drying, add vinyltriethoxysilane equivalent to 3-5% of solid weight, stir evenly, dry, and crush into powder,
[0036] Process the above-mentioned substances that have been weighed into finished aerated bricks according to the follow...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com