Method for producing high carbon steel through double-slag high drawing carbon tapping
A high-carbon steel and high-drawing carbon technology, which is applied in the field of high-carbon steel production by double-slag method high-drawing carbon tapping, can solve the problems of low production efficiency and serious phosphorus return, so as to increase the furnace life and reduce the amount of phosphorus return , Improve the effect of dephosphorization rate
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0029] According to the method for producing high-carbon steel by double slag method high-drawing carbon tapping of the present invention, 185 tons of molten iron and 23.5 tons of scrap steel are added to a 210-ton converter, and the conditions of the molten iron are: 4.13%C, 0.37%Si, 0.23%Mn , 0.10%P, 0.038%S, 1357℃; the first stage uses 2.8Nm 3 / min / t oxygen supply intensity blowing, the position of the blowing gun is 2.5 meters, the position of the process gun is 2.7-2.1 meters, and the position of the carbon pulling gun is 1.9 meters. After the blowing is started, 5 tons of lime (25 kg / tons of steel), 1.5 tons of ore (7 kg / ton of steel), the bottom blowing nitrogen flow rate is 0.1Nm 3 / min / t, the composition and temperature of molten iron at the end of the first stage are: 3.53%C, 0.002%Si, 0.09%Mn, 0.021%P, 0.041%S, 1387℃; the second stage uses 3.3Nm 3 / min / t oxygen supply intensity blowing, the blowing gun position is 2.3 meters, the process gun position is 2.6-2.1 me...
Embodiment 2
[0031] According to the method for producing high-carbon steel by double-slag method high-drawing carbon tapping of the present invention, add 183 tons of molten iron and 25 tons of scrap steel into a 210-ton converter, and the conditions of the molten iron are: 4.03%C, 0.58%Si, 0.21%Mn , 0.097%P, 0.034%S, 1377℃; the first stage uses 2.8Nm 3 / min / t of oxygen supply intensity blowing, the position of the blowing gun is 2.4 meters, the position of the process gun is 2.6-2.1 meters, the position of the carbon pulling gun is 1.8 meters, and 4.5 tons of lime (23 kg / tons of steel), 1.5 tons of ore (7 kg / ton of steel), the bottom blowing nitrogen flow rate is 0.1Nm 3 / min / t, the composition and temperature of molten iron at the end of the first stage are: 3.68%C, 0.002%Si, 0.08%Mn, 0.023%P, 0.035%S, 1369℃; the second stage uses 3.3Nm 3 / min / t oxygen supply intensity blowing, the blowing gun position is 2.3 meters, the process gun position is 2.7-2.0 meters, the blowing gun position...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com