Phosphate controlled-release fertilizer with sterilizing effect and preparation method thereof
A bactericidal effect and slow-release fertilizer technology, which is applied to organic fertilizers, excretion fertilizers, fertilization devices, etc., can solve the problems of blank production and application of slow-release fertilizers, and few slow-release fertilizers, and achieve excellent chemical stability. The effect of loss and not easy to agglomerate
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0046] 1. The composition of raw materials in molar percentage is:
[0047] P 2 o 5 47%, K 2 O is 26%, CaO is 6%, MgO is 5%, Fe 2 o 3 5%, MnO 2 4%, CuO 4%, Y 2 o 3 1%, Sm 2 o 3 1%, La 2 o 3 1%.
[0048] 2. Preparation method:
[0049] (1) take each raw material according to the molar percentage of each component;
[0050] (2) Fully mix the raw materials taken;
[0051] (3) Put the mixed mixture into a crucible, then put it into an electric furnace with a furnace temperature of 1000° C., and keep it warm for 60 minutes;
[0052] (4) Pour the melted glass liquid into a tablet press and press into thin slices or pour into cold water;
[0053] (5) Put flake or granular glass together into a ball mill for ball milling;
[0054] (6) Sieve, test and pack the ball-milled glass powder.
[0055] 3. Test results:
[0056]
Embodiment 2
[0058] 1. The composition of raw materials in molar percentage is:
[0059] P 2 o 5 34%, K 2 O is 36%, CaO is 7%, MgO is 5%, Fe 2 o 3 6%, MnO 2 4%, CuO 3%, Y 2 o 3 2%, Sm 2 o 3 2%, La 2 o 3 1%.
[0060] 2. Preparation method:
[0061] (1) take each raw material according to the molar percentage of each component;
[0062] (2) Fully mix the raw materials taken;
[0063] (3) Put the mixed mixture into a crucible, then put it into an electric furnace with a furnace temperature of 1100° C., and keep it warm for 70 minutes;
[0064] (4) Pour the melted glass liquid into a tablet press and press into thin slices or pour into cold water;
[0065] (5) Put flake or granular glass together into a ball mill for ball milling;
[0066] (6) Sieve, test and pack the ball-milled glass powder.
[0067] 3. Test results:
[0068]
Embodiment 3
[0070] 1. The composition of raw materials in molar percentage is:
[0071] P 2 o 5 38%, K 2 O is 32%, CaO is 7%, MgO is 4%, Fe 2 o 3 8%, MnO 2 3%, CuO 4%, Y 2 o 3 1%, Sm 2 o 3 1%, La 2 o 3 2%.
[0072] 2. Preparation method:
[0073] (1) take each raw material according to the molar percentage of each component;
[0074] (2) Fully mix the raw materials taken;
[0075] (3) Put the mixed mixture into a crucible, then put it into an electric furnace with a furnace temperature of 1200 ° C, and keep it warm for 50 minutes;
[0076] (4) Pour the melted glass liquid into a tablet press and press into thin slices or pour into cold water;
[0077] (5) Put flake or granular glass together into a ball mill for ball milling;
[0078] (6) Sieve, test and pack the ball-milled glass powder.
[0079] 3. Test results:
[0080]
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com