A technology of solid wood veneer and metal doors, applied in the field of metal doors, can solve problems such as difficult to achieve environmental coordination and consistency, poor wear resistance and scratch resistance, discomfort and fatigue, and achieve good elasticity, The facade is wear-resistant and scratch-resistant, and the home environment is consistent and harmonious
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0029] Embodiment 1: A pressed and surface-treated iron plate is used as the base material of the door panel, and 0.18MM ash veneer is used as the solid wood veneer material. Use one-component adhesive, use rubber roller to apply glue, and the amount of glue applied is 280~360g / m 2 1. After applying glue to the door panel, cover the veneer on the iron plate and send it to the cold press. The upper and lower surfaces of the door panel are made of particle board as a backing plate. The applied pressure is 0.6 to 0.8mPa, and pressurized at room temperature for 6-8 hours. After the pressure is released, use sandpaper to gently polish the glue bumps extruded from the brown eyes of the wood by the pressure. After polishing, spray paint and surface protection processing.
Embodiment 2
[0030] Embodiment 2: A pressed and surface-treated aluminum plate is used as the base material of the door panel, and 0.8MM gold silk teak veneer is used as the solid wood veneer material. Two-component adhesive is used, and a plastic scraper with sawtooth is used to scrape the glue, and the amount of glue applied is 300~380g / m 2After applying the glue to the door panel, cover the veneer on the iron plate and send it to the cold press. The upper and lower surfaces of the door panel are made of particle board as the backing plate, and the pressure applied is 0.6 to 0.8mPa. After 4~5 hours, after the pressure is released, use sandpaper to gently polish the glue bumps extruded from the brown eyes of the wood by the pressure, and then send it to the hot press machine. The particle board is also used as the backing board, and the applied pressure is 0.6 to 0.8mPa. , continue to pressurize at 80 degrees for 10 minutes, after the pressure is released, the surface can be painted.
PUM
Property | Measurement | Unit |
---|---|---|
thickness | aaaaa | aaaaa |
thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com