Non-halogen flame-retarding reinforced PBT plastic
A plastic, weight percent technology, applied in the field of halogen-free flame retardant reinforced PBT plastics, can solve the problems of poor mechanical properties, damage to mechanical properties, poor coloring, etc., and achieve good mechanical properties, high elongation at break, and good electrical properties. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0010] Get polybutylene terephthalate 48kg, y-(2,3 glycidoxy) propyltrimethoxysilane 0.5kg, resorcinol bisphosphate 10kg, melamine pyrophosphate 10kg, ethylene-acrylic acid Methyl ester-glycidyl methacrylate copolymer 2kg, tetrakis [3-(3,5-di-tert-butyl-4-hydroxyphenyl) propionic acid] pentaerythritol ester 0.5kg, glass fiber 30kg are standby, poly Butylene glycol phthalate is dried at 100-120°C for 4-5 hours, and then mixed according to the proportion (except glass fiber) to obtain a mixture. The fibers are successively fed into different feeding ports of the twin-screw extruder, melted and blended, extruded and granulated to obtain the halogen-free flame-retardant reinforced PBT plastic of the present invention.
Embodiment 2
[0012] Get polybutylene terephthalate 43kg, y-(2,3 glycidoxy) propyltrimethoxysilane 0.7kg, resorcinol bisphosphate 10kg, melamine pyrophosphate 15kg, ethylene-acrylic acid Methyl ester-glycidyl methacrylate copolymer 5kg, tetrakis [3-(3,5-di-tert-butyl-4-hydroxyphenyl) propionate] pentaerythritol 0.3kg, glass fiber 30kg are standby, poly Butylene glycol phthalate is dried at 100-120°C for 4-5 hours, and then mixed according to the proportion (except glass fiber) to obtain a mixture. The fibers are successively fed into different feeding ports of the twin-screw extruder, melted and blended, extruded and granulated to obtain the halogen-free flame-retardant reinforced PBT plastic of the present invention.
Embodiment 3
[0014] Get polybutylene terephthalate 45kg, y-(2,3 glycidoxy) propyltrimethoxysilane 0.6kg, resorcinol bisphosphate 10kg, melamine pyrophosphate 10kg, ethylene-acrylic acid Methyl ester-glycidyl methacrylate copolymer 5kg, tetrakis [3-(3,5-di-tert-butyl-4-hydroxyphenyl) propionate] pentaerythritol 0.4kg, glass fiber 30kg are standby, poly Butylene glycol phthalate is dried at 100-120°C for 4-5 hours, and then mixed according to the proportion (except glass fiber) to obtain a mixture. The fibers are successively fed into different feeding ports of the twin-screw extruder, melted and blended, extruded and granulated to obtain the halogen-free flame-retardant reinforced PBT plastic of the present invention.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com