Aqueous flexible plate printing ink and preparation thereof
A flexographic printing and ink technology, which is applied in the field of water-based flexographic printing ink and its preparation, can solve the problems of difficult to meet high-quality printing, printing roller corrosion, low color saturation, etc., and achieves easy decolorization and drying speed Fast, color-saturated effects
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment approach 1
[0019] According to the formula, the weight is 35% pigment, 30% acrylic resin, 0.2% defoamer, 3.8% ethylene glycol methyl ether, 1.8% wax slurry, 1.2% leveling agent, 28% water. Put the pigments in the mixer, and slowly add the acrylic resin while stirring at a low speed until the acrylic resin is completely dissolved; the dissolved mixture is ground in a sand mill so that the fineness of the color paste is less than or equal to 15 microns; the ground Put the color paste in the agitator at high speed, and neutralize until the pH value is 8.5-9.5; then add acrylic emulsion, defoamer, wax, leveling agent and water to the water-based color paste in sequence, Stir and mix evenly, adjust the viscosity with water to 40-80 seconds, and measure at 25°C with a domestic Tushi 4# cup.
[0020] The prepared ink is subjected to the following tests:
[0021] 1. Viscosity test
[0022] Instruments used: domestic Tushi 4# cup, electronic stopwatch, thermometer, ice water
[0023] Steps:
...
Embodiment approach 2
[0043] According to the formula, the weight is 33% pigment, 29% acrylic resin, 0.3% defoamer, 4.7% ethylene glycol methyl ether, 1.6% wax paste, 1.4% leveling agent, 30% water. Put the pigments in the mixer, and slowly add the acrylic resin while stirring at a low speed until the acrylic resin is completely dissolved; the dissolved mixture is ground in a sand mill so that the fineness of the color paste is less than or equal to 15 microns; the ground Put the color paste in the agitator at high speed, and neutralize until the pH value is 8.5-9.5; then add acrylic emulsion, defoamer, wax, leveling agent and water to the water-based color paste in sequence, Stir and mix evenly, adjust the viscosity with water to 40-80 seconds, and measure at 25°C with a domestic Tushi 4# cup.
[0044] The inspection method of each parameter is as described in Embodiment 1.
Embodiment approach 3
[0046] According to the formula, the weight is 32% pigment, 29% acrylic resin, 0.5% defoamer, 4.5% ethylene glycol methyl ether, 2.5% wax slurry, 1.5% leveling agent, 30% water. Put the pigments in the mixer, and slowly add the acrylic resin while stirring at a low speed until the acrylic resin is completely dissolved; the dissolved mixture is ground in a sand mill so that the fineness of the color paste is less than or equal to 15 microns; the ground Put the color paste in the agitator at high speed, and neutralize until the pH value is 8.5-9.5; then add acrylic emulsion, defoamer, wax, leveling agent and water to the water-based color paste in sequence, Stir and mix evenly, adjust the viscosity with water to 40-80 seconds, and measure at 25°C with a domestic Tushi 4# cup.
[0047] The inspection method of each parameter is as described in Embodiment 1.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com