Zinc replenisher with control released zinc and its preparing method and use
A slow-release zinc and zinc supplement technology, which is applied in the direction of medical preparations, applications, and pharmaceutical formulas containing active ingredients, can solve problems such as environmental pollution and low biological utilization, and achieve convenient use, easy promotion and implementation, The effect of high surface activity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0025] 1) Grinding a commercially available ZSM-5 zeolite molecular sieve to 300 mesh, adding water and stirring evenly to make a suspension slurry with a concentration of 5%;
[0026] 2) Slowly add zinc chloride with a zinc content of 5% by weight of zeolite into the suspension slurry in step 1) under stirring, detect and adjust the pH value of the slurry to 4.5, and react at room temperature for 6 hours;
[0027] 3) The pH value of the detection step 2) is adjusted with a 10moL / L aqueous sodium hydroxide solution to make the pH value of the slurry 7.5; washed with water for 3 times, filtered and dehydrated;
[0028] 4) The filter cake obtained in step 3) is dried and crushed to 300 meshes to obtain a controlled-release zinc supplement, and the content of zinc in the zeolite is 5% by weight percentage.
[0029] The 28-day-old weaned piglets of "Du Dachang" three-way hybridization were used as the test object, and the effects of controlled and slow-release zinc on the growth a...
Embodiment 2
[0035]Preparation: Mesoporous molecular sieve MCM-41 was prepared according to the method of "Modification and Characterization of Mesoporous Molecular Sieve MCM-41 under Mild Conditions" (Zheng Shan, Gao Lian, Guo Jingkun. Journal of Inorganic Materials, 2000, 15(5): 844-848). 41.
[0036] 1) Grind the mesoporous molecular sieve MCM-41 obtained in the preparatory step to 300 mesh, add water and stir evenly, and make a suspension slurry with a concentration of 1%;
[0037] 2) Slowly add zinc nitrate with a zinc content of 10% by weight of MCM-41 into the suspension slurry in step 1) under stirring, detect and adjust the pH value of the slurry to 6.5, and react at room temperature for 10 hours;
[0038] 3) The pH value of the detection step 2) is adjusted with 5moL / L potassium hydroxide aqueous solution, so that the pH value of the slurry is 8.5; washed 5 times with water, and centrifuged for dehydration;
[0039] 4) The filter cake obtained in step 3) was dried and crushed to...
Embodiment 3
[0047] 1) Grinding the clinoptilolite produced in Jinyun, Zhejiang to 500 mesh, adding water and stirring evenly to make a suspension slurry with a concentration of 10%;
[0048] 2) Slowly add zinc acetate with a zinc content of 2% by weight of zeolite into the suspension slurry in step 1) under stirring, detect and adjust the pH value of the slurry to 3.0, and react at room temperature for 4 hours;
[0049] 3) The pH value of the detection step 2) is adjusted with 0.5moL / L sodium carbonate aqueous solution, so that the pH value of the slurry is 7.0; washed 4 times, filtered and dehydrated;
[0050] 4) The filter cake obtained in step 3) is dried and crushed to 600 meshes to obtain a controlled-release zinc supplement, and the content of zinc in the zeolite is 2% by weight percentage.
[0051] Effects of controlled and sustained-release zinc on growth and endocrine of broiler chickens:
[0052] The effect of controlled and slow-release zinc on the growth and endocrine of broi...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com