preparation example Construction
[0033] The preparation method of above-mentioned pesticide water dispersion soft granule comprises the following steps:
[0034] 1. Mix the botanical pesticide in the formula with the carrier of the water-insoluble substance and then ultrafinely pulverize it to 500 mesh to make a botanical pesticide mixture;
[0035] Or directly spray the extract of botanical pesticides on the carrier of water-insoluble substances that have been ultrafinely pulverized to 500 meshes to make plant pesticide adsorbents;
[0036] 2. Mix the chemical pesticide or the above-mentioned botanical pesticide mixture or plant pesticide adsorbate with the wetting agent and disintegrating agent in the formula to obtain the mixed material;
[0037] 3. In addition, heat the adhesive poloxamer to 60℃~70℃ to make it melt, add it to the mixture, stir for 10~20min under the condition of high-speed shear stirring, and the stirring speed is 500~800r / min, gradually After cooling to room temperature, the pesticide w...
Embodiment 1
[0039] Embodiment 1: 20g of toosendanin coarse powder (containing 2.5% of toosendanin) and 70g of carrier urea are mixed uniformly, and ultrafinely pulverized; after pulverization, mix with wetting agent sodium lauryl sulfate 5g, and additionally poloxane Heat 5 g of mol to 60°C. After the poloxamer is melted, add it to the mixture of toosendanin coarse powder, urea and sodium lauryl sulfate, and stir with a high-speed shearer for 20 minutes at a temperature of 60°C. The speed of the stirrer is 500r / min, 100g of 0.5% toosendanin water-dispersible soft granules can be prepared.
[0040] The determination methods of various quality indicators are as follows:
[0041] 1g of the prepared 0.5% toosendanin water-dispersible soft granules was added to 99g of 342ppm standard hard water at a temperature of 30°C. Within 2.5min, the granules could disperse automatically to form a uniform emulsion; The emulsion continued to stand at a temperature of 30°C for 1 hour. There was no floating...
Embodiment 2
[0044] Example 2: 10 g of ultrafine pulverized diflubenzuron (content 99%) and 40 g of potassium carbonate as a carrier, 32 g of bentonite as a disintegrating agent and 8 g of wetting agent Pingpingjia are uniformly mixed, preheated to 54 ° C, and added 10 g of poloxamer in a molten state at 65°C was stirred at 550 r / min for 10 min. 100 g of 10% diflubenzuron water-dispersible soft granules can be obtained.
[0045]Using the determination method of various quality indicators of the preparation in Example 1, the various indicators of the prepared 10% diflubenzuron water-dispersible soft granules were measured. The measurement results are: the dispersion time in water is 2.5min, the water dispersion stability and heat storage The stability is qualified, the suspension rate of diflubenzuron is 77%, and the thermal storage decomposition rate is 1.1%.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com