A macrolide and sample processing technology, applied in measurement devices, instruments, scientific instruments, etc., can solve the problems of easy blockage of solid-phase extraction columns, failure to meet detection limit standards, and poor repeatability of test results. The effect of synergistic adsorption capacity, developed voids, and increased convenience
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0041] Example 1Fe 3 o 4 Synthesis of @ZnO&MnO powder
[0042] Add manganese sulfate, thioacetamide, zinc sulfate, ethylene glycol and isopropanol into the three-necked flask, stir for 20 minutes and mix well, then add nano-Fe 3 o 4 (100nm), in which manganese sulfate, zinc sulfate, thioacetamide and Fe 3 o 4 The mass ratio of Fe is 1:1:2.5:0.16, Fe 3 o 4 The ratio of the number of milligrams of ethylene glycol to the number of milliliters of ethylene glycol and the number of milliliters of isopropanol is 1:0.4:0.4. Stir evenly and heat to 35°C ± 5°C. Stir and react at 35°C ± 5°C for 3 days (72h) ; Transfer the reaction solution to a hydrothermal kettle, and react at a constant temperature of 200° C. for 20 hours. After the reaction solution was cooled to room temperature, it was washed several times with pure water and ethanol, and the final product was vacuum-dried at 60°C for 6 hours, and the magnetic material Fe was obtained after grinding. 3 o 4 @ZnO & MnO powder...
Embodiment 2
[0045] Example 2 Fe 3 o 4 Synthesis of @ZnO&MnO powder
[0046] Add manganese sulfate, zinc sulfate, thioacetamide, ethylene glycol and isopropanol into the three-necked flask, stir for 20 minutes and mix well, then add nano-Fe 3 o 4 (100nm), of which manganese sulfate, zinc sulfate, thioacetamide, Fe 3 o 4 The mass ratio of Fe is 1:1:2.5:0.20, Fe 3 o 4 The ratio of the milligrams of ethylene glycol to the milliliters of ethylene glycol and the milliliters of isopropanol is 1:4:4, stir evenly and heat to 35°C±5°C, stir and react at 35°C±5°C for 60h; Transfer to a hydrothermal kettle, and react at a constant temperature of 220° C. for 25 hours. After the reaction solution was cooled to room temperature, it was washed several times with pure water and ethanol, and the final product was vacuum-dried at 60°C for 6 hours, and the magnetic material Fe was obtained after grinding. 3 o 4 @ZnO & MnO powder.
[0047] Magnetic material Fe 3 o 4 The XRD characteristic diagram ...
Embodiment 3
[0050] Fe 3 o 4 @ZnO&MnO Magnetic Solid Phase Extraction (MSPE) Macrolide Antibiotics in Organic Fertilizers:
[0051] Accurately weigh 1.0g of the organic fertilizer sample in a 25mL transparent glass sample bottle, add 100mg of the magnetic material Fe of Example 1 3 o 4 Add 10mL pH=7.0Na after @ZnO&MnO powder 2 EDTA-McIlvaine buffer solution, after vortex mixing, frequency 800rpm vibration extraction and adsorption for 20min. Then the magnetic material is adsorbed by an external magnet, and the solvent and the sample are poured and discarded, and the separated Fe 3 o 4 After @ZnO&MnO powder is washed with water, it is completely immersed in 5mL of eluent composed of acetonitrile and 25% mass percent ammonia water (wherein the volume of 25% mass percent ammonia water accounts for 5% of the eluent volume, denoted as 5 % ammonia acetonitrile) at a frequency of 800 rpm for desorption for 20 minutes, the magnetic material was adsorbed and separated by an external magnet, a...
PUM
Property | Measurement | Unit |
---|---|---|
particle size | aaaaa | aaaaa |
recovery rate | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com