Embodiment 1
[0020] In this embodiment, the mineral processing tailings of a tin ore dressing field in Guangxi Zhuang Autonomous Region are collected as raw materials, and the chemical composition of the mineral processing tailings is as shown in Table 1:
[0021] Table 1 Chemical composition and content of beneficiation tailings
[0022] chemical composition SiO 2
Al 2 o 3
FeO CaO MgO As 2 o 3
PbO other Content / wt.% 65.12 4.57 10.03 5.65 3.21 1.04 0.25 10.13
[0023] Grind the tailings in the above Table 1, and collect the tailings smaller than 200 mesh. According to the mass ratio of grinding tailings: sodium hydroxide: distilled water = 1:1.5:30, mix in a 1L reactor and heat at a constant temperature at 180°C for 4 hours; after the reaction is completed, pass the reaction solution through a mesopore filter Cloth for filtration, and then centrifuged through a centrifuge to collect the supernatant, and at the same time collect the...
Embodiment 2
[0026] In this embodiment, the mineral processing tailings of a tin ore dressing field in Guangxi Zhuang Autonomous Region are collected as raw materials, and the chemical composition of the mineral processing tailings is as shown in Table 1:
[0027] Table 1 Chemical composition and content of beneficiation tailings
[0028] chemical composition SiO 2
Al 2 o 3
FeO CaO MgO As 2 o 3
PbO other Content / wt.% 65.12 4.57 10.03 5.65 3.21 1.04 0.25 10.13
[0029] Grind the tailings in the above Table 1, and collect the tailings smaller than 200 mesh. According to the mass ratio of grinding tailings: sodium hydroxide: distilled water = 1:2:20, mix in a 1L reactor, and heat at a constant temperature for 2 hours under stirring at 230°C; after the reaction is completed, pass the reaction solution through a mesopore filter Cloth for filtration, and then centrifuged through a centrifuge to collect the supernatant, and at the same ti...
PUM
Property | Measurement | Unit |
---|---|---|
particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com