Electron radiation cross-linked elastomer foam for water pump sealing and preparation method thereof
A technology of electronic radiation and water pump sealing, applied in the direction of coating, etc., can solve the problems of regulatory gaps and other issues, and achieve the effect of strong mildew resistance, fine and uniform cells, and good foaming effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0021] Prepare protein colloid, described protein colloid is the composite additive that takes zein and zein protein mass percentage 8% to be prepared by low melting point agarose and sodium xylose in container, and mixes uniformly; The proportioning ratio of additives: low melting point agarose: xylose is 1: 3; Acetyl triethyl citrate with 32% mass percentage of zein powder is added to the obtained protein mixture, and the mixture is adjusted into a uniform protein paste , use a citric acid solution with a mass fraction of 10% to adjust the pH value of the protein paste to 6.7, and use a high-speed shear dispersing emulsifier to perform emulsification treatment at a shear rate of 1000 rpm in the same direction, and the shear time is 6 minutes to obtain a protein colloid
[0022]The first step, weighing each preparation raw material by weight, 115 parts of chlorinated polypropylene, 71 parts of polyvinyl ether polymer, 41 parts of polyvinyl acetylene resin, 53 parts of solubili...
Embodiment 2
[0025] Prepare protein colloid, described protein colloid is the compound additive that takes zein and zein protein mass percentage 7% and is prepared by low-melting point agarose and sodium xylose in container, and mixes evenly; Said compound The proportioning ratio of additives: low-melting point agarose: xylose is 3: 1; Acetyl triethyl citrate with 26% mass percentage of zein powder is added to the obtained protein mixture, and the mixture is adjusted into a uniform protein paste , adjust the pH value of the protein paste to 6.0 with a citric acid solution with a mass fraction of 5-10%, and use a high-speed shear dispersing emulsifier to perform emulsification treatment at a shear speed of 600rpm in the same direction, and the shear time is 2.5min. Get protein colloids.
[0026] The first step, weighing each preparation raw material by weight, 100 parts of chlorinated polypropylene, 65 parts of polyvinyl ether polymer, 33 parts of polyvinyl acetylene resin, 47 parts of solu...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com