Embodiment 1
[0046] first part:
[0047] An antibacterial, antiviral and antifog coating film sol comprises the following raw materials in parts by weight:
[0048]
[0049] Wherein, the inorganic photocatalyst sol includes the following raw materials:
[0050]
[0051] Antibacterial ion (antibacterial silver ion): 6wt% of the tetrabutyl titanate;
[0052] The molar ratio of water and organic solvent in the inorganic photocatalyst sol system is: 1:10.5.
[0053] the second part:
[0054] A preparation method of an antibacterial and antiviral anti-fog coating sol, specifically comprising the following steps:
[0055] Step 1, preparation of inorganic photocatalyst sol
[0056] Step 1. After weighing each raw material according to the above ratio, the organic solvent is divided into two parts, that is, the first part of organic solvent and the second part of organic solvent;
[0057] Step 2. After mixing the precursor, complexing agent and the first organic solvent, stir magnetical...
Embodiment 2
[0067] first part:
[0068] An antibacterial, antiviral and antifog coating film sol comprises the following raw materials in parts by weight:
[0069]
[0070]
[0071] Wherein, the inorganic photocatalyst sol includes the following raw materials:
[0072]
[0073] Antibacterial ion (antibacterial copper ion): 4wt% of the zinc nitrate hexahydrate;
[0074] The molar ratio of water and organic solvent in the inorganic photocatalyst sol system is: 1:6.67.
[0075] the second part:
[0076] A method for preparing an antibacterial, antiviral and anti-fog coating sol, specifically comprising the following steps: the same as in Example 1.
[0077] the third part
[0078] A kind of goggles, same as embodiment 1.
Embodiment 3
[0080] first part:
[0081] An antibacterial, antiviral and antifog coating film sol comprises the following raw materials in parts by weight:
[0082]
[0083] Wherein, the inorganic photocatalyst sol includes the following raw materials:
[0084]
[0085] Antibacterial ion (antibacterial zinc ion): 3wt% of the ammonium tungstate;
[0086] The molar ratio of water and organic solvent in the inorganic photocatalyst sol system is: 1:8.5.
[0087] the second part:
[0088] A method for preparing an antibacterial, antiviral and anti-fog coating sol, specifically comprising the following steps: the same as in Example 1.
[0089] the third part
[0090] A kind of goggles, same as embodiment 1.
PUM
Property | Measurement | Unit |
---|---|---|
antibacterial rate | aaaaa | aaaaa |
transmittivity | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com